结构型材-平板(间苯)

结构型材-平板(间苯)

价格面议

发起询价


欢迎询价。

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Flat structural shape product diagram

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Flat

Thickness*Width


Thickness*Width


FP32A

3.2*1000

6.18

1/8" x 39"

13.6

FP32B

3.2*1220

7.42

1/8" x 48"

16.4

FP40A

4*800

6.2

3/16" x 32"

13.7

FP40B

4*1200

9.19

3/16" x 48"

20.3

FP48

4.8*1000

9.3

3/16" x 39"

20.5

FP50A

5*440

4.25

3/16" x 17"

9.37

FP50B

5*1220

11.8

3/16" x 48"

26

FP64

6.4*1220

14.84

1/4" x 48"

32.7

FP95

9.5*1220

22.02

3/8" x 48"

48.6

FP127

12.7*1220

29.44

1/2" x 48"

64.9

FP160

16*1220

37.2

5/8" x 48"

82

FP190

19*1220

44.1

3/4" x 48"

97.2

FP254

25.4*1220

59

1" x 48"

130

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

  Application:  

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Structural Profile - Flat Panel (Isophthalic) is commonly used in chemical platforms, trench covers, walkway treads and large-span load-bearing applications, suitable for industrial environments with requirements for corrosion resistance and strength. If you need to confirm applicability based on specific working conditions, you are welcome to contact us to discuss the usage conditions.

Selection Guide

During selection, first confirm the panel thickness and width, then make a comprehensive judgment based on load bearing, span and installation method; when necessary, it can be adapted to on-site construction through cutting, drilling and other methods. For specific specifications and size comparisons, you are welcome to contact us for detailed information.

Product Advantages

This flat panel is made of glass fiber reinforced material and an isophthalic resin system, combining good physical strength and corrosion resistance, suitable for high-strength, large-span usage requirements. For performance under different usage environments, you are welcome to confirm further with us.

Inquiry Guide

If you have requirements for the specifications, quantity or delivery of Structural Profile - Flat Panel (Isophthalic), you are welcome to contact us for detailed specifications and quotations. We will provide a corresponding solution based on your project situation.

Operating Environment

  • These FRP structural flat profiles are suitable for both indoor and outdoor installations, including industrial plants, chemical processing areas, and outdoor walkway or platform construction where moisture and weather exposure are present.
  • The isophthalic resin matrix and glass fiber reinforcement allow the profiles to resist corrosive media commonly found in chemical, marine, and wastewater environments, making them a practical choice where steel would require frequent maintenance.
  • They perform reliably across a broad temperature range typical of industrial service conditions, and, being non-conductive, they are appropriate for applications near electrical equipment or in areas requiring thermal insulation.
  • For specific chemical exposure, UV intensity, or temperature extremes at your site, contact us with your operating conditions so we can confirm the appropriate resin formulation and profile selection.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送