Structural Profiles - Flat Panel (Isophthalic)
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Flat | Thickness*Width | Thickness*Width | ||
FP32A | 3.2*1000 | 6.18 | 1/8" x 39" | 13.6 |
FP32B | 3.2*1220 | 7.42 | 1/8" x 48" | 16.4 |
FP40A | 4*800 | 6.2 | 3/16" x 32" | 13.7 |
FP40B | 4*1200 | 9.19 | 3/16" x 48" | 20.3 |
FP48 | 4.8*1000 | 9.3 | 3/16" x 39" | 20.5 |
FP50A | 5*440 | 4.25 | 3/16" x 17" | 9.37 |
FP50B | 5*1220 | 11.8 | 3/16" x 48" | 26 |
FP64 | 6.4*1220 | 14.84 | 1/4" x 48" | 32.7 |
FP95 | 9.5*1220 | 22.02 | 3/8" x 48" | 48.6 |
FP127 | 12.7*1220 | 29.44 | 1/2" x 48" | 64.9 |
FP160 | 16*1220 | 37.2 | 5/8" x 48" | 82 |
FP190 | 19*1220 | 44.1 | 3/4" x 48" | 97.2 |
FP254 | 25.4*1220 | 59 | 1" x 48" | 130 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Structural Profile - Flat Panel (Isophthalic) is commonly used in chemical platforms, trench covers, walkway treads and large-span load-bearing applications, suitable for industrial environments with requirements for corrosion resistance and strength. If you need to confirm applicability based on specific working conditions, you are welcome to contact us to discuss the usage conditions.
Selection Guide
During selection, first confirm the panel thickness and width, then make a comprehensive judgment based on load bearing, span and installation method; when necessary, it can be adapted to on-site construction through cutting, drilling and other methods. For specific specifications and size comparisons, you are welcome to contact us for detailed information.
Product Advantages
This flat panel is made of glass fiber reinforced material and an isophthalic resin system, combining good physical strength and corrosion resistance, suitable for high-strength, large-span usage requirements. For performance under different usage environments, you are welcome to confirm further with us.
Inquiry Guide
If you have requirements for the specifications, quantity or delivery of Structural Profile - Flat Panel (Isophthalic), you are welcome to contact us for detailed specifications and quotations. We will provide a corresponding solution based on your project situation.
Operating Environment
- These FRP structural flat profiles are suitable for both indoor and outdoor installations, including industrial plants, chemical processing areas, and outdoor walkway or platform construction where moisture and weather exposure are present.
- The isophthalic resin matrix and glass fiber reinforcement allow the profiles to resist corrosive media commonly found in chemical, marine, and wastewater environments, making them a practical choice where steel would require frequent maintenance.
- They perform reliably across a broad temperature range typical of industrial service conditions, and, being non-conductive, they are appropriate for applications near electrical equipment or in areas requiring thermal insulation.
- For specific chemical exposure, UV intensity, or temperature extremes at your site, contact us with your operating conditions so we can confirm the appropriate resin formulation and profile selection.