Reforming Catalyst Series: Energy-Saving Steam Reforming Catalyst with Supporting Industrial Products and Technical
Energy conservation catalyst
Primary reforming catalyst
low water-carbon ratio conversion catalyst is sintering type gaseous hydrocarbon steam-reforming energy conservation catalyst taking nickel as active constituent, aluminium oxide as carrier, rare earth oxide as promoter. I it used at upper half of reaction tube of steaming eformer furnace under operation condition of low water-carbon ratio. It is also used in full furnace.
Related Products & Services
Besides the reforming catalyst series, Greenlogy TEC also offers the following product lines and industrial technical services for various industrial applications.
FRP / Fiberglass Products
Molded FRP grating, pultruded profiles, handrails, walkways, platforms and stair treads for diverse industrial environments.
Steel Grating & Wire Rope
Steel grating and wire rope products for industrial platforms, walkways and lifting applications.
Industrial Technical Services
Including DCS control systems, industrial software (ERP/CRM) and website engineering to support factory automation and digital management.
For more product details, please feel free to contact our team.
Frequently Asked Questions
What are the active component and carrier of this reforming catalyst?
The catalyst uses nickel as the active component, aluminium oxide as the carrier, and rare earth oxide as a promoter. It is a sintering-type gaseous hydrocarbon steam-reforming energy conservation catalyst.
Under what operating conditions and loading positions is this catalyst used?
It is designed for steam reforming furnaces operating under low water-carbon ratio conditions, and is typically loaded in the upper half of the reaction tube. It can also be used in the full furnace.
What specifications and shapes are available?
Two six-hole cylindrical types are offered: short type with dimensions Φ16×9×3.2 mm and long type with Φ16×16×3.2 mm. The appearance is black and gray.
What are the strength specifications of the catalyst?
The short type has an even crushing strength of not less than 250 N per piece, while the long type is not less than 350 N per piece. These values help maintain particle integrity during industrial loading and operation.
How does the catalyst perform at 800°C and 520°C?
According to the specification table, the short type has no listed activity at 800°C and an activity at 520°C of not more than 66; the long type has an activity at 800°C of not more than 23, with no value listed at 520°C. Please confirm the specific test conditions with our technical team.
What related products and services does Greenlogy TEC offer?
Besides the reforming catalyst series, Greenlogy TEC also offers FRP/fiberglass products such as molded grating, pultruded profiles, handrails, walkways, platforms and stair treads, as well as steel grating and wire rope products, and industrial technical services including DCS control systems, industrial software (ERP/CRM) and website engineering.
| Appearance | Specification mm | Bulk specific weight kg/L | NiO % content | SiO2 % content | Fe2O3 % content | Even crushing strength N/piece | Activity at 800℃ | Activity at 520℃ |
| black and gray color | Φ16×9×3.2 6 hole (short type) | 0.90-1.10 | ≥14.00 | ≤0.30 | ≤0.35 | ≥250 | ≤66 | |
| black and gray color | Φ16×16×3.2 6 hole (long type) | 0.90-1.10 | ≥14.00 | ≤0.30 | ≤0.35 | ≥350 | ≤23 |
简体中文