    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

T-shaped steel

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

T-shaped steel

A*B*T


A*B*T



54*6*31*6

0.89

9/4" x 1/4" x 19/16" x 1/4"

1.96

54*5*45*6

1.03

9/4" x 3/16" x 7/4" x 1/4"

2.27

54*6*45*6

1.1

9/4" x 1/4" x 7/4" x 1/4"

2.43

60*6*46*6

1.3

19/8" x 1/4" x 19/16" x 1/4"

2.87

78*6.4*44.5*6

1.38

3" x 1/4" x 7/4" x 1/4"

3.04

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

 Excludes Round Rod and Square Bar 

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

FRP T-profiles are commonly used for supports and beam-column connections requiring high strength and long spans, platform framing, and structural components in corrosive environments such as chemical and marine applications. Their glass fiber reinforcement and resin system make them suitable for replacing certain metal profiles, particularly in applications with high insulation and corrosion resistance requirements. Please contact us to confirm suitability for your specific project based on load and media conditions.

Selection Guide

When selecting, first clarify the cross-sectional dimensions (A*B*T), span, load type and service environment, then use the specification table on this page for preliminary screening. If you have special requirements for corrosion resistance grade, connection method or moment of inertia, please contact us for detailed specifications and selection advice.

Product Advantages

FRP T-profiles use glass fiber as reinforcement and resin as matrix, formed by molding or pultrusion. They feature light weight, high strength, corrosion resistance, insulation and ease of processing. Compared with metal profiles of the same specification, they offer lower long-term maintenance costs and are suitable for outdoor and corrosive environments with durability requirements.

Inquiry Guide

For complete specifications, cross-section drawings, samples or bulk supply solutions, please contact us for detailed specifications and quotations. Please provide the required cross-sectional dimensions, quantity and service environment, and we will match suitable T-profile products for you accordingly.

Operating Environment

  • The pultruded FRP T-shaped steel profile is produced with glass fiber reinforcement and resin as the adhesive, and the vinyl-based resin matrix is formulated for service in chemically aggressive surroundings such as industrial plants and processing areas.
  • Because the fiberglass-reinforced composite does not corrode like structural metal, this T-shaped profile is suited to outdoor installations exposed to rain, humidity and salt-laden coastal air, as well as to indoor areas with high moisture.
  • The profile can be used in structural framing, supports and bracing where repeated contact with acids, alkalis or other corrosive media occurs, and where wash-down or splash exposure is routine.
  • For operating temperature ranges, chemical resistance ratings and other environment-specific engineering data, contact Greenlogy TEC with the intended service conditions so the suitable profile configuration can be confirmed.

立即联系我们,我们将有专业人员为您服务。

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send