结构型材-T型钢(乙烯基)
发起询价
欢迎询价。
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
T-shaped steel | A*B*T | A*B*T | ||
54*6*31*6 | 0.89 | 9/4" x 1/4" x 19/16" x 1/4" | 1.96 | |
54*5*45*6 | 1.03 | 9/4" x 3/16" x 7/4" x 1/4" | 2.27 | |
54*6*45*6 | 1.1 | 9/4" x 1/4" x 7/4" x 1/4" | 2.43 | |
60*6*46*6 | 1.3 | 19/8" x 1/4" x 19/16" x 1/4" | 2.87 | |
78*6.4*44.5*6 | 1.38 | 3" x 1/4" x 7/4" x 1/4" | 3.04 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
FRP T-profiles are commonly used for supports and beam-column connections requiring high strength and long spans, platform framing, and structural components in corrosive environments such as chemical and marine applications. Their glass fiber reinforcement and resin system make them suitable for replacing certain metal profiles, particularly in applications with high insulation and corrosion resistance requirements. Please contact us to confirm suitability for your specific project based on load and media conditions.
Selection Guide
When selecting, first clarify the cross-sectional dimensions (A*B*T), span, load type and service environment, then use the specification table on this page for preliminary screening. If you have special requirements for corrosion resistance grade, connection method or moment of inertia, please contact us for detailed specifications and selection advice.
Product Advantages
FRP T-profiles use glass fiber as reinforcement and resin as matrix, formed by molding or pultrusion. They feature light weight, high strength, corrosion resistance, insulation and ease of processing. Compared with metal profiles of the same specification, they offer lower long-term maintenance costs and are suitable for outdoor and corrosive environments with durability requirements.
Inquiry Guide
For complete specifications, cross-section drawings, samples or bulk supply solutions, please contact us for detailed specifications and quotations. Please provide the required cross-sectional dimensions, quantity and service environment, and we will match suitable T-profile products for you accordingly.
Operating Environment
- The pultruded FRP T-shaped steel profile is produced with glass fiber reinforcement and resin as the adhesive, and the vinyl-based resin matrix is formulated for service in chemically aggressive surroundings such as industrial plants and processing areas.
- Because the fiberglass-reinforced composite does not corrode like structural metal, this T-shaped profile is suited to outdoor installations exposed to rain, humidity and salt-laden coastal air, as well as to indoor areas with high moisture.
- The profile can be used in structural framing, supports and bracing where repeated contact with acids, alkalis or other corrosive media occurs, and where wash-down or splash exposure is routine.
- For operating temperature ranges, chemical resistance ratings and other environment-specific engineering data, contact Greenlogy TEC with the intended service conditions so the suitable profile configuration can be confirmed.