FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
I-beam | A*B*T1*T2 | A*B*T1*T2 | ||
IB32 | 15*32*6.4*4 | 0.51 | 9/16" x 5/4" x 1/4" x 3/16" | 1.12 |
IB38A | 30*38*3*3 | 0.53 | 19/16" x 3/2" x 1/8" x 1/8" | 1.17 |
IB45A | 45*9*180*12 | 5.4 | 7/4" x 3/8" x 7" x 1/2" | 11.9 |
IB50A | 50*102*6.4*6.4 | 2.4 | 2" x 4" x 1/4" x 1/4" | 5.29 |
IB50B | 50*102*8*8 | 3 | 2" x 4" x 5/16" x 5/16" | 6.61 |
IB76A | 76*152*6.4*6.4 | 3.59 | 3" x 6" x 1/4" x 1/4" | 7.91 |
IB76B | 76*152*9.5*9.5 | 5.32 | 3" x 6" x 3/8" x 3/8" | 11.73 |
IB102A | 102*203*9.5*9.5 | 7.2 | 4" x 8" x 3/8" x 3/8" | 15.87 |
IB102B | 102*203*12.7*12.7 | 9.5 | 4" x 8" x 1/2" x 1/2" | 20.94 |
IB120 | 120*240*12*12 | 10.5 | 19/4" x 19/2" x 1/2" x 1/2" | 23.15 |
IB127A | 127*254*9.5*9.5 | 9 | 5" x 10" x 3/8" x 3/8" | 19.84 |
IB127B | 127*254*12.7*12.7 | 11.9 | 5" x 10" x 1/2" x 1/2" | 26.24 |
IB127C | 127*152*9.5*9.5 | 7.1 | 5" x 6" x 3/8" x 3/8" | 15.65 |
IN127D | 127*152*12.7*12.7 | 9.2 | 5" x 6" x 1/2" x 1/2" | 20.28 |
IB152A | 152*305*9.5*9.5 | 10.7 | 6" x 12" x 3/8" x 3/8" | 23.68 |
IB152B | 152*305*12.7*12.7 | 14.3 | 6" x 12" x 1/2" x 1/2" | 31.53 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
This product is suitable for applications requiring strength, corrosion resistance and electrical insulation, such as chemical platforms, marine engineering, power facilities, wastewater treatment and general structural support. Contact us to learn more about application cases and suitable solutions.
Selection Guide
Selection should take into account factors such as load conditions, span, corrosive environment and connection method. We can recommend suitable specifications and resin systems based on your specific working conditions; please provide detailed parameters so that we can assist with selection.
Product Advantages
This I-beam uses an orthophthalic resin system, offering good mechanical properties, corrosion resistance and electrical insulation, and is lightweight and easy to install. Formed by the pultrusion process, it has a high fiber content and stable, reliable performance.
Inquiry Guide
For detailed specifications, technical data or customized solutions, please contact us. We can provide professional support and quotations according to project requirements.
Operating Environment
- This FRP I-beam, molded from glass fiber reinforced material with resin as the adhesive, is suitable for both indoor and outdoor structural applications where moisture and humidity are present.
- The composite construction resists corrosion from typical industrial atmospheres and many chemical media, making it appropriate for use in plants, walkways and platforms where steel would require frequent maintenance.
- As a non-conductive material, it can be used in areas where electrical insulation is a consideration.
- For specific temperature limits, chemical resistance data or exposure conditions, contact us with your project requirements.