结构型材-工字梁 (邻苯)

结构型材-工字梁 (邻苯)

价格面议

发起询价


欢迎询价。

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.   

I-beam

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

I-beam

A*B*T1*T2


A*B*T1*T2


IB32

15*32*6.4*4

0.51

9/16" x 5/4" x 1/4" x 3/16"

1.12

IB38A

30*38*3*3

0.53

19/16" x 3/2" x 1/8" x 1/8"

1.17

IB45A

45*9*180*12

5.4

7/4" x 3/8" x 7" x 1/2"

11.9

IB50A

50*102*6.4*6.4

2.4

2" x 4" x 1/4" x 1/4"

5.29

IB50B

50*102*8*8

3

2" x 4" x 5/16" x 5/16"

6.61

IB76A

76*152*6.4*6.4

3.59

3" x 6" x 1/4" x 1/4"

7.91

IB76B

76*152*9.5*9.5

5.32

3" x 6" x 3/8" x 3/8"

11.73

IB102A

102*203*9.5*9.5

7.2

4" x 8" x 3/8" x 3/8"

15.87

IB102B

102*203*12.7*12.7

9.5

4" x 8" x 1/2" x 1/2"

20.94

IB120

120*240*12*12

10.5

19/4" x 19/2" x 1/2" x 1/2"

23.15

IB127A

127*254*9.5*9.5

9

5" x 10" x 3/8" x 3/8"

19.84

IB127B

127*254*12.7*12.7

11.9

5" x 10" x 1/2" x 1/2"

26.24

IB127C

127*152*9.5*9.5

7.1

5" x 6" x 3/8" x 3/8"

15.65

IN127D

127*152*12.7*12.7

9.2

5" x 6" x 1/2" x 1/2"

20.28

IB152A

152*305*9.5*9.5

10.7

6" x 12" x 3/8" x 3/8"

23.68

IB152B

152*305*12.7*12.7

14.3

6" x 12" x 1/2" x 1/2"

31.53

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

Application:  

    Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.    

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

 Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

This product is suitable for applications requiring strength, corrosion resistance and electrical insulation, such as chemical platforms, marine engineering, power facilities, wastewater treatment and general structural support. Contact us to learn more about application cases and suitable solutions.

Selection Guide

Selection should take into account factors such as load conditions, span, corrosive environment and connection method. We can recommend suitable specifications and resin systems based on your specific working conditions; please provide detailed parameters so that we can assist with selection.

Product Advantages

This I-beam uses an orthophthalic resin system, offering good mechanical properties, corrosion resistance and electrical insulation, and is lightweight and easy to install. Formed by the pultrusion process, it has a high fiber content and stable, reliable performance.

Inquiry Guide

For detailed specifications, technical data or customized solutions, please contact us. We can provide professional support and quotations according to project requirements.

Operating Environment

  • This FRP I-beam, molded from glass fiber reinforced material with resin as the adhesive, is suitable for both indoor and outdoor structural applications where moisture and humidity are present.
  • The composite construction resists corrosion from typical industrial atmospheres and many chemical media, making it appropriate for use in plants, walkways and platforms where steel would require frequent maintenance.
  • As a non-conductive material, it can be used in areas where electrical insulation is a consideration.
  • For specific temperature limits, chemical resistance data or exposure conditions, contact us with your project requirements.