Structural Profiles - Hook Plate (Orthophthalic)
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Hook plate | A*B*T | A*B*T | ||
| 9*70*3.2(Hypotenuse) | 0.48 | 1" x 1" x 1/8" (Hypotenuse) | 1.06 | |
| 25*60*3 | 0.5 | 1" x 19/8" x 1/8" | 1.1 | |
| 25*50*3(75°) | 0.45 | 1" x 2" x 1/8" (75°) | 0.99 | |
| 30*70*4(90°) | 0.75 | 19/16" x 11/4" x 3/16" (90°) | 1.65 | |
| 30*70*3.2(90°) | 0.7 | 19/16" x 11/4" x 1/8" (90°) | 1.54 | |
| 30*90*3(87°) | 0.72 | 19/16" x 7/2" x 1/8" (87°) | 1.59 | |
| 38*230*3.2(87°) | 1.65 | 3/2" x 9" x 1/8" (87°) | 3.64 | |
| 40*254*6.4(87°) | 3.55 | 25/16" x 10" x 1/4" (87°) | 7.83 | |
| 50*140*3.2(87°) | 1.19 | 2" x 11/2" x 1/8" (87°) | 2.62 | |
| 55*152*3.6(87°) | 1.55 | 9/4" x 6" x 1/8" (87°) | 3.42 | |
| 55*230*3.6(87°) | 2.14 | 9/4" x 9" x 1/8" (87°) | 4.72 | |
| 55*205*3.2(87°) | 1.62 | 9/4" x 8" x 1/8" (87°) | 3.57 | |
| 55*55*3.2(87°) | 0.8 | 9/4" x 9/4" x 1/8" (87°) | 1.76 | |
| 55*70*3.2(87°) | 0.9 | 9/4" x 11/4" x 1/8" (87°) | 1.98 | |
| 30*76*3 | 0.6 | 19/16" x 3" x 1/8" | 1.32 | |
| 30*76*4 | 0.8 | 19/16" x 3" x 3/16" | 1.76 | |
| 25*50*3.2(90°) | 0.45 | 1" x 2" x 1/8" (90°) | 0.99 | |
| 25*50*4(90°) | 0.51 | 1" x 2" x 3/16" (90°) | 1.12 | |
| 25*100*3.2(87°) | 0.75 | 1" x 4" x 1/8" (87°) | 1.65 | |
| Fillet | 30*75*3.5 | 0.69 | 19/16" x 3" x 1/8" | 1.52 |
| Fillet | 30*100*3.2 | 0.8 | 19/16" x 4" x 1/8" | 1.76 |
| Right angle | 30*100*3.2 | 0.85 | 19/16" x 4" x 1/8" | 1.87 |
| 30*152*3.2 | 1.2 | 19/16" x 6" x 1/8" | 2.65 | |
| Fillet | 30*230*3.2 | 1.6 | 19/16" x 9" x 1/8" | 3.53 |
| Right angle | 30*230*3.2 | 1.7 | 19/16" x 9" x 1/8" | 3.75 |
| 55*300*4(90°) | 2.8 | 9/4" x 12" x 3/16" (90°) | 6.17 | |
| 55*345*4(87°) | 3.25 | 9/4" x 27/2" x 3/16" (87°) | 7.17 | |
| 30*381*3.2(87°) | 2.7 | 19/16" x 15" x 1/8" (87°) | 5.95 | |
| 55*400*3.2 | 2.8 | 9/4" x 63/4" x 1/8" | 6.17 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
FRP hook plates are commonly used for structural support and connection in corrosive environments such as chemical, wastewater treatment, and marine engineering, and are also suitable for applications requiring insulation and non-magnetic properties. Installation is flexible, and they can be cut, drilled, and otherwise processed according to actual working conditions.
Selection Guide
When selecting, factors such as load requirements, span, corrosive environment, and connection method should be considered. It is recommended to determine dimensions and specifications based on specific project needs. Please contact us for detailed specifications and selection advice.
Product Advantages
FRP hook plates feature light weight, high strength, corrosion resistance, insulation, non-magnetic properties, and easy installation. Compared with traditional metal materials, they can significantly reduce maintenance costs.
Inquiry Guidance
For detailed specifications, prices, and other commercial terms, please contact us for a customized quotation and technical support.
Operating Environment
- This FRP hook plate is a pultruded glass fiber reinforced profile with resin as the adhesive and glass fiber cloth as the reinforcement layer, so it is suited to both indoor and outdoor installations where steel alternatives would need frequent repainting.
- The closed, resin-rich surface makes the hook plate a practical choice in humid or damp plant areas and in atmospheres carrying mild corrosive media, where the profile is used as a connecting and support element rather than a decorative trim.
- Because it is produced as a structural shape for high-strength, large-span situations, the hook plate is typically specified in chemical, water treatment, marine and general industrial environments, as well as in walkway, platform and handrail assemblies.
- Service temperature range, chemical resistance ratings against specific media and UV exposure allowance depend on the resin system and the actual installation; please contact us for the parameter list that applies to your project.
简体中文