结构型材-钩子板(邻苯)

结构型材-钩子板(邻苯)

价格面议

发起询价


欢迎询价。

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Hook plate

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Hook plate

A*B*T


A*B*T



9*70*3.2(Hypotenuse)0.48

1" x 1" x 1/8" (Hypotenuse)

1.06

25*60*30.5

1" x 19/8" x 1/8"

1.1

25*50*3(75°)0.45

1" x 2" x 1/8" (75°)

0.99

30*70*4(90°)0.75

19/16" x 11/4" x 3/16" (90°)

1.65

30*70*3.2(90°)0.7

19/16" x 11/4" x 1/8" (90°)

1.54

30*90*3(87°)0.72

19/16" x 7/2" x 1/8" (87°)

1.59

38*230*3.2(87°)1.65

3/2" x 9" x 1/8" (87°)

3.64

40*254*6.4(87°)3.55

25/16" x 10" x 1/4" (87°)

7.83

50*140*3.2(87°)1.19

2" x 11/2" x 1/8" (87°)

2.62

55*152*3.6(87°)1.55

9/4" x 6" x 1/8" (87°)

3.42

55*230*3.6(87°)2.14

9/4" x 9" x 1/8" (87°)

4.72

55*205*3.2(87°)1.62

9/4" x 8" x 1/8" (87°)

3.57

55*55*3.2(87°)0.8

9/4" x 9/4" x 1/8" (87°)

1.76

55*70*3.2(87°)0.9

9/4" x 11/4" x 1/8" (87°)

1.98

30*76*30.6

19/16" x 3" x 1/8"

1.32

30*76*40.8

19/16" x 3" x 3/16"

1.76

25*50*3.2(90°)0.45

1" x 2" x 1/8" (90°)

0.99

25*50*4(90°)0.51

1" x 2" x 3/16" (90°)

1.12

25*100*3.2(87°)0.75

1" x 4" x 1/8" (87°)

1.65
Fillet30*75*3.50.69

19/16" x 3" x 1/8"

1.52
Fillet30*100*3.20.8

19/16" x 4" x 1/8"

1.76
Right angle30*100*3.20.85

19/16" x 4" x 1/8"

1.87

30*152*3.21.2

19/16" x 6" x 1/8"

2.65
Fillet30*230*3.21.6

19/16" x 9" x 1/8"

3.53
Right angle30*230*3.21.7

19/16" x 9" x 1/8"

3.75

55*300*4(90°)2.8

9/4" x 12" x 3/16" (90°)

6.17

55*345*4(87°)3.25

9/4" x 27/2" x 3/16" (87°)

7.17

30*381*3.2(87°)2.7

19/16" x 15" x 1/8" (87°)

5.95

55*400*3.22.8

9/4" x 63/4" x 1/8"

6.17

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

FRP hook plates are commonly used for structural support and connection in corrosive environments such as chemical, wastewater treatment, and marine engineering, and are also suitable for applications requiring insulation and non-magnetic properties. Installation is flexible, and they can be cut, drilled, and otherwise processed according to actual working conditions.

Selection Guide

When selecting, factors such as load requirements, span, corrosive environment, and connection method should be considered. It is recommended to determine dimensions and specifications based on specific project needs. Please contact us for detailed specifications and selection advice.

Product Advantages

FRP hook plates feature light weight, high strength, corrosion resistance, insulation, non-magnetic properties, and easy installation. Compared with traditional metal materials, they can significantly reduce maintenance costs.

Inquiry Guidance

For detailed specifications, prices, and other commercial terms, please contact us for a customized quotation and technical support.

Operating Environment

  • This FRP hook plate is a pultruded glass fiber reinforced profile with resin as the adhesive and glass fiber cloth as the reinforcement layer, so it is suited to both indoor and outdoor installations where steel alternatives would need frequent repainting.
  • The closed, resin-rich surface makes the hook plate a practical choice in humid or damp plant areas and in atmospheres carrying mild corrosive media, where the profile is used as a connecting and support element rather than a decorative trim.
  • Because it is produced as a structural shape for high-strength, large-span situations, the hook plate is typically specified in chemical, water treatment, marine and general industrial environments, as well as in walkway, platform and handrail assemblies.
  • Service temperature range, chemical resistance ratings against specific media and UV exposure allowance depend on the resin system and the actual installation; please contact us for the parameter list that applies to your project.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送