Structural Profiles - Hollow Profile (Isophthalic)
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Hollow board | A1*T1*A2*T2*B*T3 | A1*T1*A2*T2*B*T3 | ||
| 500*6*450*6*48.5*6 | 16.4 | 20" x 1/4" x 18" x 1/4" x 2" x 1/4" | 36.2 | |
| 500*6*450*6*48.5*9 | 18.5 | 20" x 1/4" x 18" x 1/4" x 2" x 3/8" | 40.8 | |
| 650*13*550*13*98.5*12 | 52.5 | 51/2" x 1/2" x 173/8" x 1/2" x 4" x 1/2" | 116 | |
| 725*4.5*675*4.5*45*4.5 | 17.9 | 57/2" x 3/16" x 53/2" x 3/16" x 7/4" x 3/16" | 39.5 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Structural Profiles - Hollow Profile (Isophthalic) is suitable for load-bearing and supporting structures with requirements on strength and span, such as platform walkways, stair treads, handrails, cable tray supports, and frame members in corrosive environments such as chemical, marine engineering, and municipal applications. Its hollow cross-section maintains section stiffness while facilitating joining and drilled installation. To confirm whether it is suitable for your specific scenario, please contact us with your working conditions.
Selection Guide
During selection, first determine the section height and wall thickness based on span, load, and support method, then choose the drilling or joining solution according to the connection form of the installation joint; the isophthalic resin system is suitable for environments with high corrosion resistance requirements and can be further discussed based on media and temperature conditions. The specifications listed on the page are common references; for actual dimensions, weight, and mechanical parameters, please refer to the detailed specifications and quotation obtained by contacting us.
Product Advantages
This profile uses glass fiber as reinforcement and resin as matrix, and is formed by impregnation, heating, compression molding, and continuous pultrusion. It features lightweight, high strength, corrosion resistance, non-magnetic, electrical insulation, and ease of processing, cutting, and drilling. The hollow profile structure achieves a larger sectional moment of inertia with equal material usage, making it suitable for high-strength, large-span support needs. Please contact us for material system and process descriptions.
Inquiry Guidance
If you need to confirm requirements such as cross-section dimensions, length, color, surface treatment, and packaging and transportation, please contact us for detailed specifications and quotations. We will recommend suitable specifications and supply solutions based on your project conditions. Bulk procurement, custom cross-sections, and technical selection support can all be discussed together.
简体中文