Structural Profiles - H-Beam (Vinyl Ester)
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
H beam | A*B*T1*T2 | A*B*T1*T2 | ||
HB76 | 76*76*6.4*6.4 | 2.67 | 3" x 3" x 1/4" x 1/4" | 5.73 |
HB102A | 102*102*6.4*6.4 | 3.59 | 4" x 4" x 1/4" x 1/4" | 7.91 |
HB102B | 102*102*8*8 | 4.5 |
4" x 4" x 5/16" x 5/16" | 9.92 |
HB152A | 152*152*6.4*6.4 | 5.43 |
6" x 6" x 1/4" x 1/4" | 11.97 |
HB152B | 152*152*9.5*9.5 | 8.1 |
6" x 6" x 3/8" x 3/8" | 17.86 |
HB203A | 203*203*9.5*9.5 | 10.8 |
8" x 8" x 3/8" x 3/8" | 23.81 |
HB203B | 203*203*12.7*12.7 | 14.4 |
8" x 8" x 1/2" x 1/2" | 31.66 |
HB203C | 203*203*6.4*6.4 | 7.5 |
8" x 8" x 1/4" x 1/4" | 16.53 |
HB254A | 254*254*9.5*9.5 | 13.6 |
10" x 10" x 3/8" x 3/8" | 29.98 |
HB254B | 254*254*12.7*12.7 | 18 |
10" x 10" x 1/2" x 1/2" | 39.77 |
HB305 | 305*305*12.7*12.7 | 21.5 |
12" x 12" x 1/2" x 1/2" | 47.4 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Vinyl H-beams are suitable for applications requiring both corrosion resistance and structural strength, such as load-bearing and support structures in chemical, water treatment, marine engineering, offshore platforms and various corrosive environments. Their long-span, high-strength characteristics also make them suitable for platform walkways, equipment supports and frame systems. For suitability under specific working conditions, please contact us so we can evaluate based on your actual service conditions.
Selection Guidance
When selecting, please first confirm the cross-sectional dimensions (A*B*T1*T2), span, load-bearing method and corrosiveness of the medium, then determine the connection and fixing scheme according to installation conditions. Different cross-sectional specifications differ in stiffness and self-weight, and must be matched to the actual stress state. For calculation recommendations and specification comparison, please contact us for detailed specifications and quotations.
Product Advantages
The product uses fiberglass as reinforcement and resin as matrix, and is formed by impregnation, mold pressing, heating and curing, and pultrusion, offering good physical properties and stable cross-sectional consistency. The vinyl system performs well in corrosion resistance, and also features light weight, high strength, and ease of cutting, processing and on-site installation. Compared with traditional metal profiles, it is more suitable for long-term use in humid and corrosive environments.
Inquiry Guidance
For business information such as specifications, dimensional tolerances, colors, surface treatment, packaging and transportation of vinyl H-beams, please contact us. Please provide the required cross-section, quantity and service environment, and we will provide detailed specifications and quotations accordingly, and assist in confirming the delivery scheme.