  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

H beam

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

H beam

A*B*T1*T2


A*B*T1*T2


HB76

76*76*6.4*6.4

2.67

3" x 3" x 1/4" x 1/4"

5.73

HB102A

102*102*6.4*6.4

3.59

4" x 4" x 1/4" x 1/4"

7.91

HB102B

102*102*8*8

4.5

4" x 4" x 5/16" x 5/16"

9.92

HB152A

152*152*6.4*6.4

5.43

6" x 6" x 1/4" x 1/4"

11.97

HB152B

152*152*9.5*9.5

8.1

6" x 6" x 3/8" x 3/8"

17.86

HB203A

203*203*9.5*9.5

10.8

8" x 8" x 3/8" x 3/8"

23.81

HB203B

203*203*12.7*12.7

14.4

8" x 8" x 1/2" x 1/2"

31.66

HB203C

203*203*6.4*6.4

7.5

8" x 8" x 1/4" x 1/4"

16.53

HB254A

254*254*9.5*9.5

13.6

10" x 10" x 3/8" x 3/8"

29.98

HB254B

254*254*12.7*12.7

18

10" x 10" x 1/2" x 1/2"

39.77

HB305

305*305*12.7*12.7

21.5

12" x 12" x 1/2" x 1/2"

47.4

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

  Application:  

    Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.    

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

 Excludes Round Rod and Square Bar 

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Vinyl H-beams are suitable for applications requiring both corrosion resistance and structural strength, such as load-bearing and support structures in chemical, water treatment, marine engineering, offshore platforms and various corrosive environments. Their long-span, high-strength characteristics also make them suitable for platform walkways, equipment supports and frame systems. For suitability under specific working conditions, please contact us so we can evaluate based on your actual service conditions.

Selection Guidance

When selecting, please first confirm the cross-sectional dimensions (A*B*T1*T2), span, load-bearing method and corrosiveness of the medium, then determine the connection and fixing scheme according to installation conditions. Different cross-sectional specifications differ in stiffness and self-weight, and must be matched to the actual stress state. For calculation recommendations and specification comparison, please contact us for detailed specifications and quotations.

Product Advantages

The product uses fiberglass as reinforcement and resin as matrix, and is formed by impregnation, mold pressing, heating and curing, and pultrusion, offering good physical properties and stable cross-sectional consistency. The vinyl system performs well in corrosion resistance, and also features light weight, high strength, and ease of cutting, processing and on-site installation. Compared with traditional metal profiles, it is more suitable for long-term use in humid and corrosive environments.

Inquiry Guidance

For business information such as specifications, dimensional tolerances, colors, surface treatment, packaging and transportation of vinyl H-beams, please contact us. Please provide the required cross-section, quantity and service environment, and we will provide detailed specifications and quotations accordingly, and assist in confirming the delivery scheme.