Structural Profiles - Cooling Tower Deck (Isophthalic)
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Cooling tower deck | A*T1*B*T2 | A*T1*B*T2 | ||
| 605*3.2*28.7*5 | 5.8 | 24" x 1/8" x 9/8" x 3/16" | 12.8 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
This structural profile - cooling tower deck (isophthalic) is suitable for load-bearing and access platforms, maintenance walkways and similar environments inside cooling towers where moisture and corrosive media are present. The isophthalic resin system performs consistently in water resistance and chemical corrosion resistance, making it suitable for long-term exposure to cooling water vapor and chemical spray conditions. For specific applicable working conditions and installation methods, please contact us for detailed specifications and quotations.
Selection Guide
During selection, match the cross-sectional dimensions such as A, T1, B and T2 in the table according to the cooling tower's span, load requirements and installation node type. If it needs to be used in combination with other FRP profiles or gratings, please provide drawings or working condition parameters so that targeted recommendations can be given. Please contact us for detailed specifications and quotations.
Product Advantages
The product is made of glass fiber reinforced material and an isophthalic resin system through the pultrusion process, featuring light weight, high strength, corrosion resistance, insulation and dimensional stability. The surface can be treated for anti-slip or wear resistance as required, making on-site cutting and installation convenient and reducing long-term maintenance costs. For more performance data, please contact us for detailed specifications and quotations.
Inquiry Guide
If you need to know the specific cross-sectional dimensions, custom lengths, surface treatment and packaging and transport solutions for this cooling tower deck, please contact us for detailed specifications and quotations. Please provide your working conditions, quantity requirements and delivery location, and we will arrange technical coordination and a commercial reply as soon as possible.
Operating Environment
- Designed for cooling tower deck applications where the FRP structural profile is exposed to continuous moisture and condensing humidity; the pultruded glass fiber reinforced composite construction resists water absorption and swelling.
- Suitable for outdoor installation on cooling towers and similar industrial structures, where the isophthalic resin system provides qualitative resistance to UV exposure and weathering.
- Performs in chemically aggressive atmospheres such as those found in chemical processing and industrial cooling water systems, where the isophthalic resin offers qualitative protection against corrosive media.
- Withstands the temperature variations typical of cooling tower service, maintaining structural integrity in both hot and cold operating conditions.