   FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.   

Cooling tower deck

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Cooling tower deck

A*T1*B*T2


A*T1*B*T2



605*3.2*28.7*55.824" x 1/8" x 9/8" x 3/16"12.8

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:    

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.    

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar  

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

This structural profile - cooling tower deck (isophthalic) is suitable for load-bearing and access platforms, maintenance walkways and similar environments inside cooling towers where moisture and corrosive media are present. The isophthalic resin system performs consistently in water resistance and chemical corrosion resistance, making it suitable for long-term exposure to cooling water vapor and chemical spray conditions. For specific applicable working conditions and installation methods, please contact us for detailed specifications and quotations.

Selection Guide

During selection, match the cross-sectional dimensions such as A, T1, B and T2 in the table according to the cooling tower's span, load requirements and installation node type. If it needs to be used in combination with other FRP profiles or gratings, please provide drawings or working condition parameters so that targeted recommendations can be given. Please contact us for detailed specifications and quotations.

Product Advantages

The product is made of glass fiber reinforced material and an isophthalic resin system through the pultrusion process, featuring light weight, high strength, corrosion resistance, insulation and dimensional stability. The surface can be treated for anti-slip or wear resistance as required, making on-site cutting and installation convenient and reducing long-term maintenance costs. For more performance data, please contact us for detailed specifications and quotations.

Inquiry Guide

If you need to know the specific cross-sectional dimensions, custom lengths, surface treatment and packaging and transport solutions for this cooling tower deck, please contact us for detailed specifications and quotations. Please provide your working conditions, quantity requirements and delivery location, and we will arrange technical coordination and a commercial reply as soon as possible.

Operating Environment

  • Designed for cooling tower deck applications where the FRP structural profile is exposed to continuous moisture and condensing humidity; the pultruded glass fiber reinforced composite construction resists water absorption and swelling.
  • Suitable for outdoor installation on cooling towers and similar industrial structures, where the isophthalic resin system provides qualitative resistance to UV exposure and weathering.
  • Performs in chemically aggressive atmospheres such as those found in chemical processing and industrial cooling water systems, where the isophthalic resin offers qualitative protection against corrosive media.
  • Withstands the temperature variations typical of cooling tower service, maintaining structural integrity in both hot and cold operating conditions.