LM Sealed Comp. Wire Rope GB6x19 (9/9/1) IWRC
Request a Quote
Please feel freely to contact with us for new price .
Product Details
6x19 sealed wire rope is available with FC (fiber core) and IWRC (independent wire rope core), offering excellent breaking load characteristics and a wide range of applications. For applications requiring higher abrasion resistance, 6x19 sealed wire rope is more suitable than other 6x19 wire ropes.
Surface treatment: bright or galvanized
Standard: National standard GB/T 20118-2006

Engineering Applications
Drilling line
Elevator hoisting rope
Wire rope slings
Luffing wire rope
Hoisting rope
Crane wire rope
Sand line, core line and swabbing line
Trawl fishing / ocean sweeping
Grounding rope / ground drag rope
Oil well / oilfield
Excavator rope / scraper rope
Fishing rope
Tow rope
Breaking load
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load | Minimum breaking load | |
|---|---|---|---|---|---|
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 10 | 0.4 | 63 | 6427 | 69.8 | 7117 |
| 11 | 0.48 | 76.2 | 7776 | 84.4 | 8611 |
| 12 | 0.58 | 90.7 | 9255 | 100 | 10248 |
| 13 | 0.68 | 106 | 10862 | 118 | 12027 |
| 14 | 0.78 | 124 | 12597 | 137 | 13949 |
| 16 | 1.02 | 161 | 16453 | 179 | 18219 |
| 18 | 1.3 | 204 | 20824 | 226 | 23059 |
| 20 | 1.6 | 252 | 25708 | 279 | 28468 |
| 22 | 1.94 | 305 | 31107 | 338 | 34447 |
| 24 | 2.3 | 363 | 37020 | 402 | 40994 |
| 26 | 2.7 | 426 | 43448 | 472 | 48111 |
| 28 | 3.14 | 494 | 50389 | 547 | 55798 |
| 30 | 3.6 | 567 | 57845 | 628 | 64054 |
| 32 | 4.1 | 645 | 65814 | 715 | 72879 |
| 34 | 4.62 | 728 | 74298 | 807 | 82274 |
| 36 | 5.18 | 817 | 83296 | 904 | 92238 |
| 38 | 5.78 | 910 | 92809 | 1008 | 102771 |
| 40 | 6.4 | 1008 | 102835 | 1116 | 113874 |
| 42 | 7.06 | 1112 | 113376 | 1231 | 125546 |
General Engineering Wire Rope
Greenlogy TEC specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 in various specifications with fiber core and steel core. In addition to these conventional wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and abrasion. All our wire ropes strive to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Each wire rope can be supplied with fittings such as thimbles, swaged ends and wedge sockets, as well as many other assembly components. We also offer custom services: our engineering team can manufacture wire rope to your required specifications. All materials are certified, traceable and conform to ISO9001.
Selection Guide
The 6x19 compacted wire rope is produced to national standard GB/T 20118-2006 and is available with FC (fiber core) and IWRC (independent wire rope core), with a bright or galvanized surface. For selection, you may consider the diameter, construction and strength grade required for your specific working conditions; please contact us for detailed specifications and quotations.
Product Advantages
This construction offers excellent breaking load characteristics and is more wear-resistant than other 6x19 wire ropes, making it suitable for applications with higher wear-resistance requirements. Its applications cover drilling lines, elevator hoist ropes, slings, luffing ropes, crane ropes and oilfield ropes, among other engineering uses.
Inquiry Guide
For parameter details corresponding to different diameters, core types and surface treatments, or to confirm supply and commercial terms, please contact us for detailed specifications and quotations. Please provide your application details and required specifications, and we will recommend a suitable product solution.
Operating Environment
- The GB6x19 (9/9/1) IWRC construction, with its independent wire rope core, suits outdoor and indoor duty where the rope is exposed to weather and repeated bending, such as drilling line, crane rope and luffing rope.
- Because the 6x19 sealed rope resists abrasion better than other 6x19 wire ropes, it is used in dusty, gritty or continuously rubbing service, including sand line, core line and swabbing line in oilfield work.
- Choose the bright finish for dry indoor hoisting such as elevator hoisting rope and slings, or the galvanized finish where atmospheric moisture and mild outdoor exposure must be withstood.
- Trawl fishing and ocean sweeping place the rope in a marine atmosphere; confirm the correct surface treatment with us before ordering for such service.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.
简体中文
English