6x19 sealed construction is a wire rope construction with superb breaking load characteristics and is used in a wide range of applications, available with both FC (fibre core) and IWRC (independent wire rope core). For applications that require higher wear resistance, 6x19 sealed wire ropes are more suitable than other 6x19 wire ropes.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Drilling ropes
Elevator rope
Wire rope slings
Derricking ropes
Pendant ropes
Crane rope
Sand, coring and swabbing lines
Trawl wraps / Pelagic sweeps
Ground cables
Oil well / Oil field
Excavator rope / Scraper rope
Fishing rope
Drag ropes
Breaking Loads
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads | |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 10 | 0.4 | 63 | 6427 | 69.8 | 7117 |
| 11 | 0.48 | 76.2 | 7776 | 84.4 | 8611 |
| 12 | 0.58 | 90.7 | 9255 | 100 | 10248 |
| 13 | 0.68 | 106 | 10862 | 118 | 12027 |
| 14 | 0.78 | 124 | 12597 | 137 | 13949 |
| 16 | 1.02 | 161 | 16453 | 179 | 18219 |
| 18 | 1.3 | 204 | 20824 | 226 | 23059 |
| 20 | 1.6 | 252 | 25708 | 279 | 28468 |
| 22 | 1.94 | 305 | 31107 | 338 | 34447 |
| 24 | 2.3 | 363 | 37020 | 402 | 40994 |
| 26 | 2.7 | 426 | 43448 | 472 | 48111 |
| 28 | 3.14 | 494 | 50389 | 547 | 55798 |
| 30 | 3.6 | 567 | 57845 | 628 | 64054 |
| 32 | 4.1 | 645 | 65814 | 715 | 72879 |
| 34 | 4.62 | 728 | 74298 | 807 | 82274 |
| 36 | 5.18 | 817 | 83296 | 904 | 92238 |
| 38 | 5.78 | 910 | 92809 | 1008 | 102771 |
| 40 | 6.4 | 1008 | 102835 | 1116 | 113874 |
| 42 | 7.06 | 1112 | 113376 | 1231 | 125546 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
6x19密封钢丝绳按国标GB/T 20118-2006生产,提供FC(纤维芯)与IWRC(独立钢丝绳芯)两种芯型,表面可为光面或镀锌。选型时可结合具体工况的直径、结构与强度等级需求,欢迎联系我们获取详细规格与报价。
产品优势
该结构具有卓越的断裂载荷特性,且相比其他6x19钢丝绳更耐磨损,适用于对耐磨性要求更高的场景。其应用覆盖钻绳、电梯升降绳、吊索、变幅绳、起重机绳及油田用绳等多种工程用途。