    Pultruded FRP profiles are a new type of composite material made with glass fiber reinforcement as the reinforcing body and resin as the binder, with glass fiber cloth as the wrapping reinforcing layer; after thorough impregnation, the material is heated, formed and cured in a metal die and then pulled by a pulling machine. With good physical properties, they are widely used in high-strength, long-span applications.   

FRP fiberglass I-beam structural profile in light gray

Type

Specification (mm)

Weight (kg/m)

Specification (in)

Weight (lbs/in)

I-beam

A*B*T1*T2


A*B*T1*T2


IB32

15*32*6.4*4

0.51

9/16" x 5/4" x 1/4" x 3/16"

1.12

IB38A

30*38*3*3

0.53

19/16" x 3/2" x 1/8" x 1/8"

1.17

IB45A

45*9*180*12

5.4

7/4" x 3/8" x 7" x 1/2"

11.9

IB50A

50*102*6.4*6.4

2.4

2" x 4" x 1/4" x 1/4"

5.29

IB50B

50*102*8*8

3

2" x 4" x 5/16" x 5/16"

6.61

IB76A

76*152*6.4*6.4

3.59

3" x 6" x 1/4" x 1/4"

7.91

IB76B

76*152*9.5*9.5

5.32

3" x 6" x 3/8" x 3/8"

11.73

IB102A

102*203*9.5*9.5

7.2

4" x 8" x 3/8" x 3/8"

15.87

IB102B

102*203*12.7*12.7

9.5

4" x 8" x 1/2" x 1/2"

20.94

IB120

120*240*12*12

10.5

19/4" x 19/2" x 1/2" x 1/2"

23.15

IB127A

127*254*9.5*9.5

9

5" x 10" x 3/8" x 3/8"

19.84

IB127B

127*254*12.7*12.7

11.9

5" x 10" x 1/2" x 1/2"

26.24

IB127C

127*152*9.5*9.5

7.1

5" x 6" x 3/8" x 3/8"

15.65

IN127D

127*152*12.7*12.7

9.2

5" x 6" x 1/2" x 1/2"

20.28

IB152A

152*305*9.5*9.5

10.7

6" x 12" x 3/8" x 3/8"

23.68

IB152B

152*305*12.7*12.7

14.3

6" x 12" x 1/2" x 1/2"

31.53

Application Markets  

FRP I-beam applications across construction and industrial markets

  • Construction

  • Bridges and Highways

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metals and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Recreation and Entertainment

  • Telecommunications

  • Transportation

  • Water and Wastewater Treatment

Features:

  • Corrosion-resistant

  • Low maintenance

  • Flame-retardant

  • Low installation cost

  • Heavy-metal resistant

  • Long service life

  • Electrically and thermally non-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame-retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

VEFR type: economical, excellent performance, resistant to moderate acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:

    Greenlogy TEC pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other costly components.    

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, longitudinal (LW)

D-638

psi

30000

kgf/m²

21092086

Tensile stress, transverse (CW)

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, longitudinal (LW)

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, transverse (CW)

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, longitudinal (LW)

D-695

psi

30000

kgf/m²

21092086

Compressive stress, transverse (CW)

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, longitudinal (LW)

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, transverse (CW)

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, longitudinal (LW)

D-790

psi

30000

kgf/m²

21092086

Flexural stress, transverse (CW)

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, longitudinal (LW)

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, transverse (CW)

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact strength, longitudinal

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact strength, transverse

D-256

ft.-lbs./in.

4

kg/m

0.55

 Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, longitudinal

D-696

10^-6in./in./℃

8

Flame-retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, longitudinal

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = longitudinal, CW = crosswise, PF = perpendicular to laminate surface

*Only applicable to ISOFR and VEFR


Application Scenarios

This product is suitable for applications requiring strength, corrosion resistance and electrical insulation, such as chemical platforms, marine engineering, power facilities, wastewater treatment and general structural support. Contact us to learn more about application cases and suitable solutions.

Selection Guide

Selection should take into account factors such as load conditions, span, corrosive environment and connection method. We can recommend suitable specifications and resin systems based on your specific operating conditions; please provide detailed parameters so that we can assist with selection.

Product Advantages

This I-beam uses an orthophthalic resin system and offers good mechanical properties, corrosion resistance and electrical insulation, along with light weight and easy installation. It is formed by the pultrusion process, with high fiber content and stable, reliable performance.

Inquiry Guidance

For detailed specifications, technical data or customized solutions, please contact us. We can provide professional support and quotations based on project requirements.

Service Environment

  • This FRP I-beam is molded from glass-fiber reinforced material with resin as the binder, and is suitable for indoor and outdoor structural applications where moisture and humidity are present.
  • The composite structure resists corrosion from typical industrial atmospheres and various chemical media, making it suitable for factories, walkways and platforms where steel requires frequent maintenance.
  • As a non-conductive material, it can be used in locations where electrical insulation needs to be considered.
  • For specific temperature limits, chemical resistance data or exposure conditions, please share your project requirements with us.