结构型材-七孔隔墙板(乙烯基)

结构型材-七孔隔墙板(乙烯基)

价格面议

发起询价


欢迎询价。

Genius FRP  

   FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.   

Seven hole partition board

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)


1000*140*531.6

39" x 11/2" x 3/16"

69.7

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

Application:  

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.  

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

The seven-hole partition panel is suitable for locations requiring clean, corrosion-resistant and lightweight partitioning, such as plant and laboratory partitions in the chemical, food and beverage, and electronics manufacturing industries. Its FRP material is easy to rinse and clean, and it is also commonly used for internal partition walls in bridge and tunnel ancillary facilities and municipal engineering. For specific scenario adaptation recommendations, please contact us.

Selection Guidance

When selecting, it is recommended to first confirm the partition's load conditions, span, service environment (humidity, chemical exposure) and installation method, then evaluate based on the panel section dimensions and unit weight. If it needs to coordinate with existing structures, suspended ceilings, or door and window openings, please provide drawings or dimensional requirements, and we can assist in matching specifications. For detailed selection parameters, please contact us.

Product Advantages

This partition panel is made of glass fiber reinforced material composited with resin and formed by molding and pultrusion. It features high strength, light weight, corrosion resistance, insulation and maintenance-free performance, making it suitable for large spans and humid environments. The surface is flat and can be cut and drilled, allowing convenient on-site installation. For certifications and performance data, please contact us.

Inquiry Guidance

If you would like to know the specifications, colors, surface treatments and supply methods of the seven-hole partition panel, please contact us for detailed specifications and quotations. Please inform us of the service environment, required dimensions and quantity, and we will provide selection recommendations and commercial terms accordingly.

Operating Environment

  • The seven-hole FRP partition panel is built from glass fiber reinforced material with resin as the adhesive and a glass fiber cloth package reinforcement layer, so it is suited to both indoor installations and outdoor structures where moisture and weather exposure are present.
  • Because the resin matrix and glass fiber reinforcement resist chemical attack, this pultruded partition panel is commonly used in chemical, food and beverage, metals and mining, and microelectronics facilities where corrosive media and washdown conditions occur.
  • The panel performs in architectural, bridge and highway, and manufacturing environments, where humidity swings and continuous service loads are part of normal operation.
  • For temperature limits, chemical resistance ratings, and the full parameter list, contact us with your project conditions.

立即联系我们,我们将有专业人员为您服务。

7*24小时的专业团队,我们将有专业人员,为您提供一对一的个性化服务。

发送