结构型材-扁管(乙烯基)
欢迎询价。
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Flat tube | A*B*T1*T2 | A*B*T1*T2 | ||
| FT44 | 44*25*3.2*3.2 | 0.8 | 7/4" x 1" x 1/8" x 1/8" | 1.76 |
| FT50A | 51*25*3*3 | 0.79 | 2" x 1" x 1/8" x 1/8" | 1.74 |
| FT50B | 51*25*6.4*6.4 | 1.54 | 2" x 1" x 1/4" x 1/4" | 3.4 |
| FT76 | 76*35*3*6 | 1.55 | 3" x 11/8" x 1/8" x 1/4" | 3.42 |
| FT80 | 80*60*5*5 | 2.5 | 25/8" x 19/8" x 3/16" x 3/16" | 5.51 |
| FT91A | 91*38*4*4 | 1.78 | 7/2" x 3/2" x 3/16" x 3/16" | 3.92 |
| FT112A | 112*91*6.4*6.4 | 4.46 | 9/2" x 7/2" x 1/4" x 1/4" | 9.83 |
| FT120 | 120*45*3*3 | 2 | 19/4" x 7/4" x 1/8" x 1/8" | 4.41 |
| FT175 | 175*50*9*9 | 7 | 55/8" x 2" x 3/8" x 3/8" | 15.4 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density |
D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
结构型材-扁管(乙烯基)广泛应用于化工、海洋、电力等对耐腐蚀要求较高的领域,常见于平台栏杆、支撑结构、走道格栅框架等。扁管截面便于连接和安装,适合需要轻质高强、绝缘无磁的场合。
选型指导
选型时请根据实际载荷、跨距及使用环境,结合扁管的截面尺寸和壁厚进行选择。我们提供多种规格,可满足不同结构需求。如需精确选型建议,欢迎联系我们获取详细规格与技术支持。
产品优势
采用乙烯基树脂,具有优异的耐腐蚀性和耐候性;玻璃纤维增强赋予其高强度、轻质的特点。拉挤工艺确保产品尺寸稳定、表面光洁,且具备绝缘、无磁、免维护等优势。
询盘引导
如需了解结构型材-扁管(乙烯基)的详细规格、价格及供货信息,欢迎联系我们获取详细规格与报价。我们的技术团队将为您提供专业选型建议和定制方案。