FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Skirting board

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Skirting boardA*B*T
A*B*T
M2100*13*3.2 M-shape1.13.94*0.51*0.13 M-shape2.43
M3100*16*5 M-shape1.33.94*0.63*0.2 M-shape2.87
M4148*12*3 M-shape1.275.83*0.47*0.12 M-shape2.8
W1100*19*5 W-shape1.363.94*0.75*0.2 W-shape3
W2100*15*3.2 W-shape1.13.94*0.59*0.13 W-shape2.43
W3150*15*3.2 W-shape1.65.91*0.59*0.13 W-shape3.53

Markets

Markets
  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Standard color

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Grass green,Yellow, Grey, Orange

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

Grass green,Yellow, Grey

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

Grass green,Yellow, Grey

General acid and alkali environment

Application:

Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638psi30000kgf/m²21092086

Tensile Stress, CW

D-638psi7000

kgf/m²

4921487

Tensile Modulus, LW

D-63810^6psi2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-63810^6psi0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695psi30000

kgf/m²

21092086

Compressive Stress, CW

D-695psi15000

kgf/m²

10546043

Compressive Modulus, LW

D-69510^6psi2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-69510^6psi1

10^6kgf/m²

703

Flexural Stress, LW

D-790psi30000

kgf/m²

21092086

Flexural Stress, CW

D-790psi10000

kgf/m²

7030695

Flexural Modulus, LW

D-79010^6psi1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-79010^6psi0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi2.8

10^6kgf/m²

1969

Shear Modulus

---10^6psi0.45

10^6kgf/m²

316

Short Beam Shear

D-2344psi4500

kgf/m²

3163813

Punch Shear

D-732psi10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256ft.-lbs./in.25kg/m3.46

Notched Izod Impact,CW

D-256ft.-lbs./in4kg/m0.55

Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495---45

24 Hour Water Absorption

D-570%max0.45

Density

D-792lbs./in.³0.062-0.07

Coefficient of Thermal Expansion,LW

D-69610^-6in./in./℃8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149kv./in.35

Dielectric Strength,PF

D-149volts/mil200

Dielectric Constant,PF

D-150@60hz5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Structural Profile - Kick Plate is commonly used in corrosive environments such as chemical platforms, wastewater treatment, marine engineering and power facilities, serving as an edge protection and kick component in combination with FRP grating and pultruded profiles. To confirm suitability for your specific working conditions, please contact us for detailed specifications and quotations.

Selection Guide

During selection, you can make an initial match from A*B*T specifications based on the dimensions of the installation surface, the required cross-sectional shape (such as M-shaped) and load-bearing requirements. As specific parameters and customization needs are involved, we recommend providing drawings or operating conditions so we can assist in recommending a suitable model. Please contact us for detailed specifications and quotations.

Product Advantages

This kick plate is pultruded from fiberglass reinforced material and resin, featuring corrosion resistance, light weight, high strength, insulation and ease of cutting and installation, making it suitable for high-humidity and chemical media environments. Different resin systems can meet various working conditions. Please contact us for detailed specifications and quotations.

Inquiry Guide

To learn about available specifications, surface treatments and bulk supply information for the Structural Profile - Kick Plate, please provide us with your dimensions, quantity and operating environment. Please contact us for detailed specifications and quotations, and we will provide a targeted solution based on your needs.