结构型材-角钢(乙烯基)
欢迎询价。
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Angle steel | A*B*T1*T2 | A*B*T1*T2 | ||
| EL25A | 25*25*3.2*3.2 | 0.33 | 1" x 1" x 1/8" x 1/8" | 0.73 |
| EL25B | 25*25*6.4*6.4 | 0.56 | 1" x 1" x 1/4" x 1/4" | 1.23 |
| EL30A | 30*30*4(75°) | 0.46 | 5/4" x 5/4" x 3/16" (75°) | 1.01 |
| EL30B | 30*30*5*5 | 0.57 | 5/4" x 5/4" x 3/16" x 3/16" | 1.26 |
| EL32 | 32*32*4*4 | 0.42 | 5/4" x 5/4" x 3/16" x 3/16" | 0.93 |
| EL38A | 38*38*5*5 | 0.68 | 3/2" x 3/2" x 3/16" x 3/16" | 1.5 |
| EL38B | 38*38*6.4*6.4 | 0.85 | 3/2" x 3/2" x 1/4" x 1/4" | 1.87 |
| EL45 | 45*45*4.8*4.8 | 0.75 | 7/4" x 7/4" x 3/16" x 3/16" | 1.65 |
| EL50A | 50*50*3.2*3.2 | 0.62 | 2" x 2" x 1/8" x 1/8" | 1.37 |
| EL50B | 50*50*6.4*6.4 | 1.14 | 2" x 2" x 1/4" x 1/4" | 2.51 |
| EL60 | 60*60*9*9 | 1.9 | 19/8" x 19/8" x 3/8" x 3/8" | 4.19 |
| EL76A | 76*76*4.8*4.8 | 1.38 | 3" x 3" x 3/16" x 3/16" | 3.04 |
| EL76B | 76*76*6.4*6.4 | 1.77 | 3" x 3" x 1/4" x 1/4" | 3.9 |
| EL76C | 76*76*9.5*9.5 | 2.57 | 3" x 3" x 3/8" x 3/8" | 5.67 |
| EL76D | 76*76*12.7*12.7 | 3.4 | 3" x 3" x 1/2" x 1/2" | 7.5 |
| EL101A | 101*101*6.4*6.4 | 2.5 | 4" x 4" x 1/4" x 1/4" | 5.51 |
| EL101B | 101*101*8*8 | 2.95 | 4" x 4" x 5/16" x 5/16" | 6.5 |
| EL101C | 101*101*9.5*9.5 | 3.48 | 4" x 4" x 3/8" x 3/8" | 7.67 |
| EL101D | 101*101*12.7*12.7 | 4.57 | 4" x 4" x 1/2" x 1/2" | 10.1 |
| EL152A | 152*152*6.4*6.4 | 3.62 | 6" x 6" x 1/4" x 1/4" | 7.98 |
| EL152B | 152*152*9.5*9.5 | 5.42 | 6" x 6" x 3/8" x 3/8" | 12 |
| EL152C | 152*152*12.7*12.7 | 7.01 | 6" x 6" x 1/2" x 1/2" | 15.5 |
| L40 | 40*22*4.0*4.0 | 0.45 | 25/16" x 7/8" x 3/16" x 3/16" | 0.99 |
| L76 | 76*15*6*6 | 0.98 | 3" x 9/16" x 1/4" x 1/4" | 2.16 |
| L100 | 100*50*6.4*6.4 | 1.8 | 4" x 2" x 1/4" x 1/4" | 3.97 |
| L145 | 145*76*10*10 | 3.85 | 23/4" x 3" x 3/8" x 3/8" | 8.49 |
| L170 | 170*76*9.5*9.5 | 4.4 | 27/4" x 3" x 3/8" x 3/8" | 9.7 |
| L180 | 180*80*8.0*8.0 | 3.89 | 7" x 25/8" x 5/16" x 5/16" | 8.58 |
| L254 | 254*40*6.4*6.4 | 3.61 | 10" x 25/16" x 1/4" x 1/4" | 7.96 |
| L70(Special) | 70*70*24*6.0 | 3.75 | 11/4" x 11/4" x 15/16" x 1/4" | 8.27 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 |
10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density |
D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
应用场景
结构型材-角钢(乙烯基)适用于化工、海洋、污水处理等腐蚀性环境中的框架支撑与连接件,也常用于平台、走道及爬梯等需要绝缘、无磁、轻质高强的场合。若您的项目对耐腐蚀或承载有特殊要求,欢迎联系我们说明工况以获取适配建议。
选型指导
选型时请根据实际受力形式、跨度及连接方式,确定角钢的截面尺寸与厚度,并结合环境介质选择树脂体系(如乙烯基)。我们可协助您评估所需规格与长度,具体尺寸、重量及供货形式请以询盘确认为准。
产品优势
该角钢采用玻璃纤维增强与树脂拉挤成型,具有轻质高强、耐腐蚀、绝缘及无磁等特点,安装便捷,适合替代部分金属角钢。与其他FRP型材组合使用时,可形成稳定的结构体系,降低维护成本。
询盘引导
如需了解结构型材-角钢(乙烯基)的详细规格、技术参数、包装及交付信息,欢迎联系我们获取详细规格与报价。请提供所需型号、数量及使用环境,我们将根据您的需求提供针对性方案。
简体中文