LM(Coating)Filler Compacted Wire Rope GB6X19 (12/6+6F/1) FC

LM(Coating)Filler Compacted Wire Rope GB6X19 (12/6+6F/1) FC

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

Product Details

 6X19 (Coating)filler compacted wire rope (often referred to as 6X25) is available with both FC (fibre core) and IWRC (independent wire rope core). 6X19 filler wire rope can work from 1 tonne  load up to 5 tonnes. It is used   in the North Sea Oil industry . 

Surface treatment:Ungalv  or  Galvanized

Standard:GB/T 20118-2006

LM Filler Compacted Wire Rope GB6X19 (12/6+6F/1) FC

Applications 

  • Drilling ropes

  • Elevator rope

  • Wire rope slings

  • Derricking ropes

  • Derricking ropes

  • Crane rope


  • Sand, coring and swabbing lines

  • Trawl wraps / Pelagic sweeps

  • Ground cables

  • Oil well / Oil field

  • Excavator rope / Scraper rope

  • Fishing rope

  • Drag ropes

Breaking Loads

Min Breaking Loads

Min Breaking Loads

Min Breaking Loads

Min Breaking Loads


Diameter

Weight 

(1770Mpa)

(1770Mpa)

(1960Mpa)

(1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

140.71141167712712930
160.921501525216616889
181.161891930321021375
201.442342383125926389
221.742832883531331931
242.073363431737338000
262.433954027443744598
282.824584670950751723
303.235265362058259376
323.685986100866267556
344.156756887274876265
364.657577721383885501
385.188438603093495265
405.74935953251035105557
426.3310301050951141116377
446.9511311153431252127724
467.612361260671369139600
488.2713461372681490152003

General Engineering Ropes

   GREENLOGY TEC(LM) specializes in supplying multiple strands of  ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.

    Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.


选型指导

该产品为LM(Coating)Filler Compacted Wire Rope GB6X19(12/6+6F/1)FC结构,绳芯为纤维芯,适用于需要一定柔韧性与承载能力的吊装及牵引场景。选型时建议结合使用工况、所需直径、破断荷载要求及表面处理方式(光面或镀锌)进行匹配,欢迎联系我们获取详细规格与报价,由技术人员协助确认适配型号。

产品优势

该钢丝绳采用压实填料结构,在保证破断荷载的同时兼顾柔韧性与抗磨损性能,表面可做光面或镀锌处理以适应不同环境。符合GB/T 20118-2006标准,常见于钻绳、电梯升降绳、吊索及起重等多类工程应用,欢迎联系我们了解具体优势与适用方案。

询盘引导

如需了解该产品的具体直径、重量、破断荷载对应参数及表面处理选项,欢迎联系我们获取详细规格与报价。请提供使用场景、所需直径及数量等信息,我们将结合需求推荐合适规格并协助完成选型。