Structural Profiles - Y-Shaped Steel (Orthophthalic)

Structural Profiles - Y-Shaped Steel (Orthophthalic)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Y-shaped steel

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Y-shaped steel

A*B*T


A*B*T



25*38*6.41.4

1" x 3/2" x 1/4"

3.09

38*38*6.41.6

3/2" x 3/2" x 1/4"

3.53

50*38*6.41.7

2" x 3/2" x 1/4"

3.75

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Y-shaped steel (orthophthalic) is commonly used in load-bearing and connection parts requiring strength and span, such as platform supports, frame joints, handrail frameworks, and structural components in corrosive environments such as chemical and water treatment. Its orthophthalic resin system is suitable for general anti-corrosion and outdoor use. For specific application suitability, please contact us for confirmation.

Selection Guide

When selecting, first confirm the load form, connection method, and installation space, then match the A*B*T cross-section dimensions and unit weight to the existing structural design. Similar specifications in the table can be substituted on the principle of equal strength or equal stiffness. Because working conditions vary greatly, we recommend providing us with the load, span, and corrosion conditions so our technical staff can assist in recommending suitable specifications.

Product Advantages

This profile uses glass fiber reinforcement and a resin matrix, and is formed by molding and pultrusion. It has the typical characteristics of composite materials such as light weight, high strength, corrosion resistance, insulation, and non-magnetic properties. It is suitable for replacing some metal profiles to reduce self-weight and lower maintenance frequency. The surface can maintain good appearance consistency and is easy to cut and drill.

Inquiry Guide

For detailed specifications, length options, packaging methods, and commercial terms of Y-shaped steel (orthophthalic), please contact us for detailed specifications and quotations. Please provide the required cross-section dimensions, quantity, and usage environment, and we will respond promptly accordingly.

Operating Environment

  • Y-shaped steel FRP structural profiles are suited to both indoor and outdoor installations, where the glass fiber reinforcement and resin matrix resist moisture and weathering without the corrosion risk of untreated metal shapes.
  • The pultruded FRP construction allows continuous service in humid, salt-laden or chemically aggressive atmospheres typical of chemical plants, water treatment works and coastal projects, where the Y profile is used as a load-bearing or bracing member.
  • Because the profile is formed by heating and curing in a metal mold and pulled by the traction machine, the finished Y-shaped steel retains its dimensional stability across the normal temperature swings of industrial service, from cold outdoor sites to warm plant interiors.
  • For specific chemical exposure, UV load or temperature limits, contact Greenlogy TEC with your project conditions and we will confirm suitability from the full parameter list.