Structural Profiles - U-Channel Square Tube Handrail Profile (Orthophthalic Resin)

Structural Profiles - U-Channel Square Tube Handrail Profile (Orthophthalic Resin)

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

Genius FRP  

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

U type tube handrail profiles

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

U type tube handrail profiles

A*B*T


A*B*T



62*59*4.51.5

5/2" x 9/4" x 3/16"

3.31

62*60*51.7

5/2" x 19/8" x 3/16"

3.75

Markets 

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

Application:  

    Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

Excludes Round Rod and Square Bar  

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

This U-channel square tube handrail profile is suitable for building railings, bridge pedestrian handrails, platform and walkway edge protection, and other applications requiring strength and corrosion resistance. Its fiberglass-reinforced structure is suitable for long-span, high-strength installation environments, and can also be used in chemical, coastal, and other projects susceptible to moisture and chemical media. Please contact us to confirm a suitable solution based on your project conditions.

Selection Guide

During selection, you can start with cross-sectional dimensions, wall thickness, and unit weight, and match them with handrail span, installation method, and load-bearing requirements. The table provides various A*B*T specifications and their corresponding weights, making it easy to do an initial screening according to structural design requirements. If you need recommendations for specific spans and loads, please contact us for detailed specifications and selection advice.

Product Advantages

This profile uses fiberglass as reinforcement and resin as binder, and is formed through impregnation, heated compression molding and curing, and pultrusion. It offers good physical properties and corrosion resistance. Compared with traditional metal profiles, it is lighter in weight, making transportation and on-site installation easier, while also being suitable for high-strength and long-span applications. Specific performance must be evaluated based on actual service conditions. Please contact us for further information.

Inquiry Guidance

If you need to confirm commercial information such as specifications, batch quantities, or lead times, please contact us for detailed specifications and quotations. Please provide the required cross-sectional dimensions, quantity, and service environment, and we will arrange follow-up communication accordingly. All commercial terms can be further negotiated according to your project requirements.

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor