Structural Profiles - Three-Cell Hollow Profile (Vinyl Ester)

Structural Profiles - Three-Cell Hollow Profile (Vinyl Ester)

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

Genius FRP  

   FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.   

Three hole hollow plate

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)


450*4.5*150*618.2

18" x 3/16" x 6" x 1/4"

40.1

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.  

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

The three-cell hollow profile (vinyl ester) is suitable for applications requiring high corrosion resistance and strength, such as chemical platforms, sewage treatment facilities, marine engineering, and building structures. Its hollow-cell design reduces self-weight while providing good load-bearing capacity, making it suitable for long-span applications. To check its suitability for a specific scenario, please contact us for detailed specifications and a quotation.

Selection Guide

When selecting a profile, consider factors such as load requirements, span, service environment (corrosiveness, temperature), and installation method. The vinyl ester resin gives the product excellent corrosion resistance, making it suitable for a wide range of chemical environments. Our technical team can help you choose the right specifications for your specific needs; please contact us for detailed specifications and a quotation.

Product Advantages

The three-cell hollow profile is made of fiberglass-reinforced material and vinyl ester resin, offering high strength, light weight, corrosion resistance, electrical insulation, and long service life. Its hollow-cell design reduces weight while maintaining mechanical performance, making it easy to transport and install. The smooth surface keeps maintenance costs low. Contact us for detailed specifications and a quotation.

Inquiry Guide

For detailed technical parameters, custom dimensions, bulk pricing, and delivery information on the three-cell hollow profile (vinyl ester), please feel free to contact us. We provide professional technical support and customization services. Contact us for detailed specifications and a quotation.

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor