Structural Profiles - T-Beam (Orthophthalic)

Structural Profiles - T-Beam (Orthophthalic)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

    FRP pultruded profiles are a new type of composite material made with glass fiber reinforcement as the base material, resin as the binder, and glass fiber cloth as the covering reinforcement layer; after thorough impregnation, they are heated, formed and cured in a metal mold and then pulled by a pultrusion machine. They offer good physical properties and are widely used in high-strength, long-span applications.  

Greenlogy TEC FRP pultruded T-shaped structural profile made of orthophthalic resin, model OFR-25

Type

Specification (mm)

Weight (kg/m)

Specification (in)

Weight (lbs/in)

T-section Steel

A*B*T


A*B*T



54*6*31*6

0.89

9/4" x 1/4" x 19/16" x 1/4"

1.96

54*5*45*6

1.03

9/4" x 3/16" x 7/4" x 1/4"

2.27

54*6*45*6

1.1

9/4" x 1/4" x 7/4" x 1/4"

2.43

60*6*46*6

1.3

19/8" x 1/4" x 19/16" x 1/4"

2.87

78*6.4*44.5*6

1.38

3" x 1/4" x 7/4" x 1/4"

3.04

Markets 

Greenlogy TEC FRP T-profile applications across various industrial markets

  • Construction

  • Bridges and Highways

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metals and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Leisure

  • Telecommunications

  • Transportation

  • Water and Wastewater Treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy-metal safe

  • Long service life

  • Non-conductive and non-heat-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardancy

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

An economical VEFR type with good performance and moderate resistance to acids, alkalis and solvents

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

Applications:  

  Greenlogy TEC pultruded FRP structural profiles are widely used in numerous fields, combining corrosion resistance, high strength, dimensional stability and light weight, along with thermal insulation and electrical insulation properties. Durable Greenlogy TEC profiles provide years of low-maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today, these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of elasticity

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

 Excluding round rods and square rods 

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Max %

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max 25

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

V/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies only to ISOFR and VEFR


Application Scenarios

As a structural section, T-section steel (orthophthalic) is commonly used for supports, frames and reinforcing structures requiring high strength and larger spans, such as platform guardrails, walkway frameworks, equipment supports and load-bearing components in corrosive environments. Its corrosion resistance, light weight and high strength make it suitable for chemical, water treatment, marine engineering and other applications with demanding weatherability requirements. For specific applicable working conditions, please contact us for detailed recommendations.

Selection Guide

During selection, match the T-section steel's cross-sectional dimensions and unit weight to the structural span, load conditions, connection method and installation environment. The orthophthalic resin system offers a balanced combination of corrosion resistance and mechanical performance, making it suitable for most general structural requirements. If you are unsure which specification to choose, please contact us for detailed specifications and a quotation, and our technical staff will assist you in confirming.

Product Advantages

This T-section steel is made of glass fiber as reinforcement and resin as binder through a pultrusion process. It features light weight, high strength, corrosion resistance, insulation and non-magnetic properties, and is easy to cut and install on site. Compared with traditional metal sections, it is easier to maintain in humid or corrosive environments. For specific performance data, please contact us for detailed specifications and a quotation.

Inquiry Guidance

For detailed specifications, dimensional tolerances, supply forms and commercial terms of the T-section steel (orthophthalic), please contact us. Please provide the required specifications, quantity and operating environment, and we will reply as soon as possible with a quotation and technical support.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp