Structural Profiles - Square Tube (Orthophthalic)
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Square tube | A*B*T1*T2 | A*B*T1*T2 | ||
| ST25A | 25*25*3.2*3.2 | 0.53 | 1" x 1" x 1/8" x 1/8" | 1.17 |
| ST25B | 25*25*6.4*6.4 | 0.9 | 1" x 1" x 1/4" x 1/4" | 1.98 |
| ST32A | 32*32*3.2*3.2 | 0.7 | 5/4" x 5/4" x 1/8" x 1/8" | 1.54 |
| ST32B | 32*32*6.4*6.4 | 1.24 | 5/4" x 5/4" x 1/4" x 1/4" | 2.73 |
| ST38A | 38*38*3.2*3.2 | 0.85 | 3/2" x 3/2" x 1/8" x 1/8" | 1.87 |
| ST38B | 38*38*5*5 | 1.25 | 3/2" x 3/2" x 3/16" x 3/16" | 2.76 |
| ST38C | 38*38*6.4*6.4 | 1.54 | 3/2" x 3/2" x 1/4" x 1/4" | 3.4 |
| ST44A | 44*44*3.2*3.2 | 1.01 | 7/4" x 7/4" x 1/8" x 1/8"
| 2.23 |
| ST44B | 44*44*6.4*6.4 | 1.83 | 7/4" x 7/4" x 1/4" x 1/4"
| 4.03 |
| ST50A | 50*50*3.2*3.2 | 1.14 | 2" x 2" x 1/8" x 1/8" | 2.51 |
| ST50B | 50*50*3.5*3.5 | 1.24 | 2" x 2" x 1/8" x 1/8" | 2.73 |
| ST50C | 50*50*4*4 | 1.42 | 2" x 2" x 3/16" x 3/16"
| 3.13 |
| ST50D | 50*50*5*5 | 1.74 | 2" x 2" x 3/16" x 3/16" | 3.84 |
| ST50E | 50*50*6.4*6.4 | 2.12 | 2" x 2" x 1/4" x 1/4" | 4.67 |
| ST54A | 54*54*3.2*3.2 | 1.24 | 9/4" x 9/4" x 1/8" x 1/8" | 2.73 |
| ST54B | 54*54*4.8*4.8 | 1.78 | 9/4" x 9/4" x 3/16" x 3/16" | 3.92 |
| ST60A | 60*60*5*5 | 2.1 | 19/8" x 19/8" x 3/16" x 3/16"
| 4.63 |
| ST64A | 64*64*3.2*3.2 | 1.48 | 5/2" x 5/2" x 1/8" x 1/8" | 3.26 |
| ST64B | 64*64*4.4*4.4 | 1.97 | 5/2" x 5/2" x 3/16" x 3/16"
| 4.34 |
| ST64C | 64*64*6.4*6.4 | 2.8 | 5/2" x 5/2" x 1/4" x 1/4"
| 6.17 |
| ST76A | 76*76*3.2*3.2 | 1.77 | 3" x 3" x 1/8" x 1/8"
| 3.9 |
| ST76B | 76*76*5*5 | 2.7 | 3" x 3" x 3/16" x 3/16" | 5.95 |
| ST76C | 76*76*6.4*6.4 | 3.39 | 3" x 3" x 1/4" x 1/4" | 7.47 |
| ST76D | 76*76*9.5*9.5 | 4.89 | 3" x 3" x 3/8" x 3/8" | 10.8 |
| ST89A | 89*89*6.4*6.4 | 3.95 | 7/2" x 7/2" x 1/4" x 1/4" | 8.71 |
| ST101A | 101*101*3.2*3.2 | 2.38 | 4" x 4" x 1/8" x 1/8"
| 5.25 |
| ST101B | 101*101*5*5 | 3.61 | 4" x 4" x 3/16" x 3/16"
| 7.96 |
| ST101C | 101*101*6.4*6.4 | 4.61 | 4" x 4" x 1/4" x 1/4" | 10.2 |
| ST152A | 152*152*6.4*6.4 | 7.1 | 6" x 6" x 1/4" x 1/4" | 15.7 |
| ST152B | 152*152*9.5*9.5 | 10.4 | 6" x 6" x 3/8" x 3/8" | 22.9 |
| ST152C | 152*152*12.7*12.7 | 13.5 | 6" x 6" x 1/2" x 1/2" | 29.8 |
| STR25 | 25*25*3.175*3.175 | 0.7 | 1" x 1" x 1/8" x 1/8" | 1.54 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Square tube structural profiles are commonly used for platform and walkway supports, handrail frames, equipment supports and large-span frames where strength and corrosion resistance are required. In corrosive environments such as chemical, water treatment and electroplating, they can replace some traditional metal profiles. Contact us to discuss suitable applications based on your specific working conditions.
Selection Guide
When selecting, first confirm the cross-section dimensions (A×B) and wall thickness (T1, T2), and evaluate them together with span, load type and support method. Different resin systems and fiber content affect mechanical performance. For specific specifications and load-bearing recommendations, contact us for detailed specifications and quotations.
Product Advantages
The square tube is pultruded from glass fiber reinforced material with resin, featuring light weight, high strength, corrosion resistance, insulation and ease of cutting and processing. The surface can be treated in different ways as needed to suit various installation methods. To learn about specific performance and process details, contact us.