Structural Profiles - Solid Round Rod (Orthophthalic)
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Solid round bar | D | D | ||
| SRR60 | 6 | 0.08 | 1/4" | 0.18 |
| SRR95 | 9.5 | 0.14 | 3/8" | 0.31 |
| SRR127 | 12.7 | 0.26 | 1/2" | 0.57 |
| SRR254 | 25.4 | 1 | 1" | 2.2 |
| SRR328 | 31.8 | 1.51 | 5/4" | 3.33 |
| SRR380 | 38 | 2.15 | 3/2" | 4.74 |
| SRR42 | 4.2 | 0.03 | 3/16" | 0.07 |
| SRR80 | 8.0 | 0.1 | 5/16" | 0.22 |
| SRR16 | 16 | 0.41 | 5/8" | 0.9 |
| SRR19 | 19 | 0.55 | 3/4" | 1.21 |
| SRR20 | 20 | 0.62 | 13/16" | 1.37 |
| SRR22 | 22 | 0.72 | 7/8" | 1.59 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Solid round rod combines high axial strength with corrosion resistance, and is commonly used in chemical platform handrails, ladder rungs, cable supports and insulating equipment structures where strength and rust resistance requirements are relatively high. If you need to confirm suitability for a specific corrosive medium or load condition, please contact us for detailed specifications and a quotation.
Selection Guide
When selecting, please first confirm the required diameter (metric or corresponding imperial sizes), the length to be used, and the type of loading (tension, compression or bending), and match these with the installation method and connector type. Our technical team can help recommend specifications based on your operating conditions. Please contact us for detailed specifications and a quotation.
Product Advantages
This product is made of glass fiber reinforcement with a resin matrix, formed by pultrusion. It offers the typical composite characteristics of light weight, high strength, corrosion resistance, insulation and low maintenance, and is suitable for replacing some metal rods to reduce long-term maintenance costs. Specific performance data is subject to the actual specification. Please contact us for detailed specifications and a quotation.
Inquiry Guide
For commercial information such as dimensional tolerances, available lengths, surface condition and packaging, please provide the required specifications, quantity and delivery destination, and we will reply as soon as possible. Please contact us for detailed specifications and a quotation.