Structural Profiles - Seven-Hole Hollow Plate (Isophthalic)
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
| 600*8.5*56*8 | 25.4 | 24" x 5/16" x 2" x 5/16" | 56 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
The seven-hole hollow plate (isophthalic) is suitable for structural and load-bearing locations requiring strength, span and corrosion resistance, such as building platforms, bridge and tunnel components, support structures in chemical and food processing environments, and walkways and frames at manufacturing and mining sites. If you need to confirm a usage scheme based on specific working conditions, please contact us to obtain detailed specifications and a quotation.
Selection Guidance
During selection, you may start from conditions such as load-bearing requirements, span, support spacing, service environment and installation method, and judge in combination with how well the isophthalic resin system matches properties such as corrosion resistance. Please inform us of your drawings or working condition parameters so that we can assist in confirming suitable specifications and configuration.
Product Advantages
This structural profile uses glass fiber reinforced material and resin as its matrix, and is formed through impregnation, hot press curing and pultrusion. It has good physical properties, is suitable for high-strength and large-span use scenarios, and is easy to cut and install on site. The above content covers general product characteristics; for specific performance data, please refer to the technical materials we provide. Please contact us to obtain detailed specifications and a quotation.
Inquiry Guidance
If you need information on the specifications, performance or supply of Structural Profile - Seven-Hole Hollow Plate (Isophthalic), please contact us and state the application scenario and required quantity, and we will provide corresponding technical support and commercial solutions accordingly. Please contact us to obtain detailed specifications and a quotation.
Operating Environment
- FRP structural shapes profile resists corrosion from acids, alkalis and salts, making it suitable for chemical processing, food and beverage plants, and other facilities where moisture or aggressive media are present.
- The glass fiber reinforced composite construction withstands outdoor exposure, including UV radiation and temperature fluctuations, for applications in architectural, bridge and highway, and metals and mining environments.
- With low thermal conductivity, the profiles help reduce heat transfer in high-humidity or condensing conditions, supporting use in microelectronics and manufacturing settings where stable performance is required.
- FRP structural shapes profile is non‑magnetic and non‑sparking, allowing safe operation near sensitive equipment or in environments where metallic materials may pose a risk.
简体中文