  FRP pultruded profiles use glass fiber as the reinforcement, resin as the adhesive, and glass fiber cloth as the wrapping reinforcement layer; after thorough impregnation, they are heated, formed and cured in a metal mold and drawn by a pulling machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

Plum blossom-shaped FRP fiberglass structural profile tube

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Quincunx tube

D1*D2*T
D1*D2*T
CT32A19*32*6.41.110.75*1.26*0.252.45
CT34A19*34*7.51.30.75*1.34*0.32.87
CT32B25*32*3.50.660.98*1.26*0.141.46
CT4229*42*6.41.351.14*1.65*0.252.98
CT45A28*45*8.51.861.1*1.77*0.334.1
CT45B32*45*6.41.11.26*1.77*0.252.43
CT5151*36*71.752.01*1.42*0.283.86
CT90B71*90*9.55.72.8*3.54*0.3712.6

Markets  

FRP fiberglass profiles market application overview

  • Construction

  • Bridges and highways

  • Chemical

  • Food and beverage

  • Manufacturing

  • Metals and mining

  • Microelectronics

  • Oil and gas

  • Pharmaceutical

  • Power

  • Pulp and paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and wastewater treatment

Features:

  • Corrosion resistance

  • Low maintenance cost

  • Flame retardant

  • Low installation cost

  • Heavy metal resistant

  • Long service life

  • Non-conductive, non-heat-conductive

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Standard color

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Grass green, yellow, gray, orange

Acid, alkali and other harsh corrosive environments

IFR-25

Isophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

An economical VEFR type with good performance and moderate acid, alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 and above

Grass green, yellow, gray

General acid and alkali environments

Applications:

  Greenlogy TEC (Nantong Greenlogy Electronic Technology Co., Ltd.) pultruded FRP profiles are widely used in various applications, combining corrosion resistance, high strength, dimensional stability and light weight with thermal insulation and non-conductive properties. Durable Greenlogy TEC (Nantong Greenlogy Electronic Technology Co., Ltd.) profiles provide years of low-maintenance service in areas traditionally using steel, aluminum or wood components. Today, these profiles are often used in highly corrosive applications that previously required stainless steel and other expensive components.  

Greenlogy TEC (Nantong Greenlogy Electronic Technology Co., Ltd.) Profiles

Mechanical Properties

ASTM

Unit

Value

Unit

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

% max.

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flame retardant performance

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Max. 25

Flame resistance*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Applications

As a type of structural profile, the FRP quincunx tube is commonly used in frameworks and support parts requiring light weight, high strength and corrosion resistance, such as platform handrails, ladders, brackets and structural components in power and chemical environments. If you need to confirm suitability for specific operating conditions, please contact us to discuss.

Selection guidance

When selecting, match the cross-section size, wall thickness and length to the loading method, span, mounting interface and corrosion resistance requirements; different specifications differ in load capacity and self-weight. For specific specifications and selection advice, please contact us for detailed specifications and quotations.

Product advantages

The FRP quincunx tube is pultruded from glass fiber reinforcement and a resin system, offering a favorable strength-to-weight ratio, corrosion resistance and electrical insulation, making it suitable for replacing some traditional metal profiles. For different resin systems and surface treatment options, please contact us to confirm.

Inquiry guidance

If you would like to know the available specifications, size ranges, supply forms and commercial terms for the FRP quincunx tube, please provide your application scenario and required quantity, and we will recommend a suitable solution accordingly. You are welcome to contact us for detailed specifications and quotations.

Operating environment

  • This pultruded FRP quincunx tube is a composite material using glass fiber as reinforcement, resin as binder and glass fiber cloth as reinforcement layer, so it is suitable for indoor and outdoor installations subject to moisture and weather exposure.
  • Cured FRP profiles can withstand humid environments and the corrosive media typical of chemical, wastewater treatment and coastal plant environments, where steel profiles require continuous protection.
  • Because the tube is formed with a closed quincunx cross-section, it is typically used as a structural member in high-strength, long-span applications such as industrial walkways, platforms and support frames.
  • To learn about the service temperature range, chemical exposure conditions or UV requirements for a specific project, please contact Greenlogy TEC with your application details so that a suitable pultruded profile can be confirmed.

Custom Cutting

Need panels that fit, or cut to shape? We custom cut FRP grating and profiles to your drawing: panels cut to size or to shape (corner cuts, cutouts), cut edges sealed with resin, and pre-cut and pre-drilled to drawing before shipping. See the custom cutting services.

WhatsApp