FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Skirting board | A*B*T | A*B*T | ||
M2 | 100*13*3.2 M-shape | 1.1 | 4" x 1/2" x 1/8" M-shape
| 2.43 |
M3 | 100*16*5 M-shape | 1.3 | 4" x 5/8" x 3/16" M-shape | 2.87 |
M4 | 148*12*3 M-shape | 1.27 | 23/4" x 1/2" x 1/8" M-shape | 2.8 |
W1 | 100*19*5 W-shape | 1.36 | 4" x 3/4" x 3/16" W-shape | 3 |
W2 | 100*15*3.2 W-shape | 1.1 | 4" x 9/16" x 1/8" W-shape | 2.43 |
W3 | 150*15*3.2 W-shape | 1.6 | 6" x 9/16" x 1/8" W-shape | 3.53 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Kick plate profiles are suitable for protection and decorative edging on industrial platforms, floor edges and in corrosive environments, and can be used with structural profile systems. In chemical plants, wastewater treatment and marine engineering applications, they provide corrosion-resistant, insulating kick plate protection and extend the service life of the base structure. Contact us to learn about specific application cases and matching solutions.
Selection Guide
Please select the cross-section shape and thickness according to the dimensions of the installation location, load-bearing requirements and environmental conditions; models such as M2, M3 and M4 correspond to different sizes. If you need custom lengths or colors, provide drawings or samples and we will assist with selection. Contact us for detailed specification sheets and technical support.
Product Advantages
FRP kick plates feature light weight, high strength, corrosion resistance, insulation and low maintenance, with a smooth, easy-to-clean surface and strong design flexibility. Compared with traditional metal materials, they last longer in humid or chemically corrosive environments and are easy to install. Contact us for samples and performance data.
Inquiry Guide
To obtain product quotations, technical parameters or customized services, please contact us through the website and provide the required model, quantity and application, and we will reply as soon as possible. You are welcome to inquire about cooperation.
Operating Environment
- FRP skirting boards are suitable for both indoor and outdoor installations, including industrial plants, walkways, and platforms.
- The glass fiber reinforced composite construction provides resistance to moisture and humidity, making it appropriate for use in damp or wet environments.
- These profiles withstand exposure to many corrosive media encountered in industrial settings, such as chemical plants and wastewater treatment facilities.
- They perform reliably across a range of ambient temperatures typical of industrial and commercial applications.