Structural Profiles - Kick Plate (Vinyl Ester)

Structural Profiles - Kick Plate (Vinyl Ester)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Greenlogy TEC

  FRP pultruded profiles are made from glass fiber reinforced material as the raw material, resin as the binder, and glass fiber cloth as the wrapping reinforcing layer; after full impregnation, they are heated, formed, and cured in a metal mold and pulled by a haul-off machine to form a new type of composite material with good physical properties, widely used in high-strength and long-span applications.  

FRP composite skirting board profile, model VEFR-25

Type

Size (mm)

Weight (kg/m)

Size (in)

Weight (lbs/in)

Kick Plate

A*B*T


A*B*T


M2

100*13*3.2 M型

1.1

4" x 1/2" x 1/8" M型

2.43

M3

100*16*5 M型

1.3

4" x 5/8" x 3/16" M型

2.87

M4

148*12*3 M型

1.27

23/4" x 1/2" x 1/8" M型

2.8

W1

100*19*5 W型

1.36

4" x 3/4" x 3/16" W型

3

W2

100*15*3.2 W型

1.1

4" x 9/16" x 1/8" W型

2.43

W3

150*15*3.2 W型

1.6

6" x 9/16" x 1/8" W型

3.53

Markets 

Applications of FRP profiles in construction, bridges and highways
  • Construction

  • Bridges and Highways

  • Chemical

  • Food and Beverage

  • Manufacturing

  • Metals and Mining

  • Microelectronics

  • Oil and Gas

  • Pharmaceutical

  • Power

  • Pulp and Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water and Wastewater Treatment

Features:

  • Corrosion resistance

  • Low maintenance

  • Flame retardant

  • Low installation cost

  • Heavy metal resistance

  • Long service life

  • Electrical and thermal insulation

  • High strength-to-weight ratio

Raw material introduction — resin types

Code

Resin type

Flame retardant performance

Recommended applications

VEFR-25

Vinyl ester type

Oxygen index 28 and above

Suitable for harsh corrosive environments such as acids and alkalis

IFR-25

Isophthalic type

Oxygen index 28 and above

The VEFR type is an economical product with good performance and moderate acid, alkali and solvent resistance

OFR-25

Orthophthalic type

Oxygen index 28 and above

General acid and alkali environments

 Applications: 

   Greenlogy TEC pultruded FRP profiles are widely used, combining corrosion resistance, high strength, dimensional stability and light weight with thermal and electrical insulation properties. Where steel, aluminum or wood members have traditionally been specified, durable Greenlogy TEC profiles offer years of low-maintenance service. Today these profiles are commonly used in highly corrosive applications that previously required stainless steel and other costly components.   

Greenlogy TEC profiles

Mechanical properties

ASTM

Unit

Value

Unit

Value

Tensile stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Elastic modulus

Full section

10^6psi

2.8

10^6kgf/m²

1969

Shear modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short-beam shear

D-2344

psi

4500

kgf/m²

3163813

Punch shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod impact, LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod impact, CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excluding round rods and square rods

Physical properties

ASTM

Unit

Value

Barcol hardness

D-495

---

45

24-hour water absorption

D-570

Maximum percentage

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of thermal expansion, LW

D-696

10^-6in./in./℃

8

Flammability

ASTM

Unit

Value

Tunnel test*

E-84

Flame spread

Maximum 25

Combustibility*

D-635

---

Non-combustible

Electrical properties

ASTM

Unit

Value

Arc resistance, LW

D-495

秒(s)

120

Dielectric strength, LW

D-149

kv./in.

35

Dielectric strength, PF

D-149

Volts/mil

200

Dielectric constant, PF

D-150

@60hz

5

LW = lengthwise, CW = crosswise, PF = perpendicular to laminate surface

*Applies to ISOFR and VEFR only


Application Scenarios

Vinyl kick plate structural profiles are commonly used for edge protection of platforms, walkways and equipment in corrosive environments such as chemical processing, electroplating and water treatment, and can be installed together with FRP grating and pultruded profiles. If you need to confirm suitability for a specific operating condition, please contact us to discuss.

Selection Guide

When selecting, consider the dimensions of the mounting surface, the required cross-sectional shape (such as M-shape), and the load-bearing and protection requirements, then choose a similar specification from the existing size chart. For non-standard sizes or special cross-section requirements, please contact us for detailed specifications and a quotation.

Product Advantages

This profile is pultruded from glass fiber reinforcement and resin, offering corrosion resistance, high strength and light weight, making it suitable for replacing some metal kick plates in damp or chemically exposed environments. Specific performance can be further discussed based on project requirements.

Inquiry Guide

To learn about detailed specifications, supply forms and commercial terms for vinyl kick plate structural profiles, please contact us for detailed specifications and a quotation. We can provide selection advice and technical support based on your application needs.

Operating Environment

  • This vinyl kick plate from the FRP pultruded profile product line is suitable for indoor and outdoor installation, resists moisture and will not expand or warp.
  • The vinyl surface provides lasting protection against routine chemical splashes and corrosive media common in industrial environments, extending service life in demanding plant conditions.
  • The kick plate maintains performance across the wide temperature range common in industrial and commercial applications, retaining its shape and structural integrity under high-temperature, low-temperature and humid conditions.
  • The profile uses a pultruded FRP core, withstanding long-term outdoor weather exposure and washdown operations, making it a practical choice for platforms, walkways and process areas.