Structural Profiles - Hook Plate (Isophthalic)

Structural Profiles - Hook Plate (Isophthalic)

¥ 1.00 1.0 CNY

¥ 1.00

Add To Cart


Please feel freely to contact with us for new price .

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Hook plate

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Hook plate

A*B*T


A*B*T



9*70*3.2(Hypotenuse)0.48

1" x 1" x 1/8" (Hypotenuse)

1.06

25*60*30.5

1" x 19/8" x 1/8"

1.1

25*50*3(75°)0.45

1" x 2" x 1/8" (75°)

0.99

30*70*4(90°)0.75

19/16" x 11/4" x 3/16" (90°)

1.65

30*70*3.2(90°)0.7

19/16" x 11/4" x 1/8" (90°)

1.54

30*90*3(87°)0.72

19/16" x 7/2" x 1/8" (87°)

1.59

38*230*3.2(87°)1.65

3/2" x 9" x 1/8" (87°)

3.64

40*254*6.4(87°)3.55

25/16" x 10" x 1/4" (87°)

7.83

50*140*3.2(87°)1.19

2" x 11/2" x 1/8" (87°)

2.62

55*152*3.6(87°)1.55

9/4" x 6" x 1/8" (87°)

3.42

55*230*3.6(87°)2.14

9/4" x 9" x 1/8" (87°)

4.72

55*205*3.2(87°)1.62

9/4" x 8" x 1/8" (87°)

3.57

55*55*3.2(87°)0.8

9/4" x 9/4" x 1/8" (87°)

1.76

55*70*3.2(87°)0.9

9/4" x 11/4" x 1/8" (87°)

1.98

30*76*30.6

19/16" x 3" x 1/8"

1.32

30*76*40.8

19/16" x 3" x 3/16"

1.76

25*50*3.2(90°)0.45

1" x 2" x 1/8" (90°)

0.99

25*50*4(90°)0.51

1" x 2" x 3/16" (90°)

1.12

25*100*3.2(87°)0.75

1" x 4" x 1/8" (87°)

1.65
Fillet30*75*3.50.69

19/16" x 3" x 1/8"

1.52
Fillet30*100*3.20.8

19/16" x 4" x 1/8"

1.76
Right angle30*100*3.20.85

19/16" x 4" x 1/8"

1.87

30*152*3.21.2

19/16" x 6" x 1/8"

2.65
Fillet30*230*3.21.6

19/16" x 9" x 1/8"

3.53
Right angle30*230*3.21.7

19/16" x 9" x 1/8"

3.75

55*300*4(90°)2.8

9/4" x 12" x 3/16" (90°)

6.17

55*345*4(87°)3.25

9/4" x 27/2" x 3/16" (87°)

7.17

30*381*3.2(87°)2.7

19/16" x 15" x 1/8" (87°)

5.95

55*400*3.22.8

9/4" x 63/4" x 1/8"

6.17

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

 Application:  

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

   Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Hook plates (isophthalic) are commonly used for edge fixing of platforms in chemical, electroplating, and wastewater treatment applications, connecting with gratings, handrails, or profiles to provide reliable support and fastening. They also deliver performance advantages in applications requiring high strength and corrosion resistance, such as marine engineering and oil platforms. Specific suitability needs to be evaluated based on actual operating conditions; contact us for application advice.

Selection Guide

When selecting, determine the hook plate dimensions (A*B*T), angle (e.g., 75° or beveled edge), and installation method to ensure compatibility with existing structures. Isophthalic resin provides better corrosion resistance than orthophthalic resin, making it suitable for more demanding chemical environments. For detailed specifications and selection support, contact us for professional advice.

Product Advantages

Made with isophthalic resin, the hook plate offers excellent corrosion resistance and mechanical strength, is lightweight, easy to install, and electrically insulating and non-magnetic. Fiberglass reinforcement ensures long-term durability, suitable for high-load and outdoor environments. We can provide customized solutions upon request; please contact us for details.

Inquiry Guide

Contact us for detailed specifications, technical parameters, and quotations. We provide professional selection support and customization services to meet your project needs. Please reach us via our website or email, and we will respond promptly.

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor