Structural Profiles - H-Beam (Isophthalic)
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
H beam | A*B*T1*T2 | A*B*T1*T2 | ||
HB76 | 76*76*6.4*6.4 | 2.67 | 3" x 3" x 1/4" x 1/4" | 5.73 |
HB102A | 102*102*6.4*6.4 | 3.59 | 4" x 4" x 1/4" x 1/4" | 7.91 |
HB102B | 102*102*8*8 | 4.5 |
4" x 4" x 5/16" x 5/16" | 9.92 |
HB152A | 152*152*6.4*6.4 | 5.43 |
6" x 6" x 1/4" x 1/4" | 11.97 |
HB152B | 152*152*9.5*9.5 | 8.1 |
6" x 6" x 3/8" x 3/8" | 17.86 |
HB203A | 203*203*9.5*9.5 | 10.8 |
8" x 8" x 3/8" x 3/8" | 23.81 |
HB203B | 203*203*12.7*12.7 | 14.4 |
8" x 8" x 1/2" x 1/2" | 31.66 |
HB203C | 203*203*6.4*6.4 | 7.5 |
8" x 8" x 1/4" x 1/4" | 16.53 |
HB254A | 254*254*9.5*9.5 | 13.6 |
10" x 10" x 3/8" x 3/8" | 29.98 |
HB254B | 254*254*12.7*12.7 | 18 |
10" x 10" x 1/2" x 1/2" | 39.77 |
HB305 | 305*305*12.7*12.7 | 21.5 |
12" x 12" x 1/2" x 1/2" | 47.4 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Structural Profile - H-Beam (Isophthalic) is suitable for applications with high requirements for corrosion resistance and strength, such as chemical platforms, wastewater treatment facilities, marine engineering, bridge walkways and long-span support structures. Its lightweight and high-strength characteristics can reduce the load on support structures and facilitate installation and maintenance.
Selection Guide
During selection, it is necessary to clarify the span, load conditions and service environment, and choose the appropriate cross-sectional dimensions based on the existing specification table. If custom cross-sections or special lengths are required, please contact us for detailed specifications and quotations.
Product Advantages
The isophthalic resin system gives the product excellent corrosion resistance and water resistance, while glass fiber reinforcement ensures high strength and stiffness. The product also features light weight, electrical insulation, non-magnetic properties and long service life, making it suitable as a replacement for traditional metal profiles.
Inquiry Guide
For detailed specifications, technical parameters or bulk purchase terms of Structural Profile - H-Beam (Isophthalic), please contact us for detailed specifications and quotations. We will provide professional advice based on your needs.
Operating Environment
- This pultruded FRP H-beam is built on an isophthalic resin system, which makes the profile suitable for continuous service in outdoor and humid industrial settings where mild acids, alkalis and salt-laden air are present.
- The glass fiber reinforcement and isophthalic resin matrix allow the H-beam to be used in chemical plants, wastewater areas and coastal installations where steel would require frequent recoating or replacement.
- Because the profile is non-conductive and corrosion-resistant, it is commonly selected for indoor and outdoor structural frames, platforms and support beams exposed to weather, moisture and process spillage.
- For applications involving concentrated chemicals, elevated temperatures or sustained load at high temperature, contact us with the specific medium and service condition so the correct resin grade and profile size can be confirmed.