FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
Flat tube | A*B*T1*T2 | A*B*T1*T2 | ||
| FT44 | 44*25*3.2*3.2 | 0.8 | 7/4" x 1" x 1/8" x 1/8" | 1.76 |
| FT50A | 51*25*3*3 | 0.79 | 2" x 1" x 1/8" x 1/8" | 1.74 |
| FT50B | 51*25*6.4*6.4 | 1.54 | 2" x 1" x 1/4" x 1/4" | 3.4 |
| FT76 | 76*35*3*6 | 1.55 | 3" x 11/8" x 1/8" x 1/4" | 3.42 |
| FT80 | 80*60*5*5 | 2.5 | 25/8" x 19/8" x 3/16" x 3/16" | 5.51 |
| FT91A | 91*38*4*4 | 1.78 | 7/2" x 3/2" x 3/16" x 3/16" | 3.92 |
| FT112A | 112*91*6.4*6.4 | 4.46 | 9/2" x 7/2" x 1/4" x 1/4" | 9.83 |
| FT120 | 120*45*3*3 | 2 | 19/4" x 7/4" x 1/8" x 1/8" | 4.41 |
| FT175 | 175*50*9*9 | 7 | 55/8" x 2" x 3/8" x 3/8" | 15.4 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density |
D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Structural Profiles - Flat Rectangular Tube (Orthophthalic) are suitable for load-bearing and support structures requiring strength and corrosion resistance, such as platform walkways, handrail systems, supports and frames. Their flat cross-section facilitates connection and installation, and they can replace some traditional metal profiles, making them suitable for corrosive environments such as chemical, water treatment and marine applications.
Selection Guide
During selection, load type, span, support conditions and service environment should be considered comprehensively to determine the appropriate cross-sectional dimensions and wall thickness. Flat rectangular tubes of different specifications differ in load-bearing capacity and stiffness. It is recommended to consult our technical personnel based on actual operating conditions to obtain suitable selection advice.
Product Advantages
This flat rectangular tube is reinforced with orthophthalic resin and glass fiber, offering good physical properties, corrosion resistance and the characteristics of being lightweight and high-strength. The pultrusion process ensures full fiber impregnation and continuous molding, giving the product stable mechanical properties and dimensional consistency, making it suitable for high-strength, large-span applications.
Inquiry Guide
For detailed specifications, dimensional tolerances, performance parameters or commercial terms (such as minimum order quantity, delivery time, etc.), please contact us to obtain detailed specifications and quotations. We can provide technical support and customized solutions according to your project requirements.