Structural Profiles - Flat Panel (Vinyl Ester)

Structural Profiles - Flat Panel (Vinyl Ester)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

    FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Flat structural shape diagram showing cross-section profile

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Flat

Thickness*Width


Thickness*Width


FP32A

3.2*1000

6.18

1/8" x 39"

13.6

FP32B

3.2*1220

7.42

1/8" x 48"

16.4

FP40A

4*800

6.2

3/16" x 32"

13.7

FP40B

4*1200

9.19

3/16" x 48"

20.3

FP48

4.8*1000

9.3

3/16" x 39"

20.5

FP50A

5*440

4.25

3/16" x 17"

9.37

FP50B

5*1220

11.8

3/16" x 48"

26

FP64

6.4*1220

14.84

1/4" x 48"

32.7

FP95

9.5*1220

22.02

3/8" x 48"

48.6

FP127

12.7*1220

29.44

1/2" x 48"

64.9

FP160

16*1220

37.2

5/8" x 48"

82

FP190

19*1220

44.1

3/4" x 48"

97.2

FP254

25.4*1220

59

1" x 48"

130

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

  Application:  

   Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.   

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

This structural profile flat panel is suitable for platforms, walkways, handrails, support beams and various load-bearing structural components that require strength, span and corrosion resistance. It can also be used as a structural alternative in corrosive environments such as chemical, marine and wastewater treatment applications. For load and span matching in specific scenarios, please contact us to discuss based on your actual working conditions.

Selection Guide

When selecting, first confirm the thickness and width specifications, then evaluate the required cross-sectional dimensions based on the load, span and corrosion conditions of the operating environment. The specifications listed in the table cover common flat panel sizes. If the existing specifications do not fully match your needs, please contact us for detailed specifications and selection recommendations.

Product Advantages

Made from glass fiber reinforcement with a resin matrix through the pultrusion process, it offers good physical properties and corrosion resistance, suitable for high-strength, long-span applications and situations where traditional materials are prone to corrosion. Compared with metal materials, it is lighter in weight, making transportation and installation easier. For specific performance parameters, please contact us for detailed information.

Inquiry Guide

For detailed specifications, pricing, supply capability and other commercial terms of this structural profile flat panel, please contact us for details and a quotation. Our team will provide corresponding support based on your application requirements.

立即联系我们,我们将有专业人员为您服务。

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send