Structural Profiles - Flat Bar

Structural Profiles - Flat Bar

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Riglet

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Riglet

Width*Thickness


Width*Thickness


FS1919*6.40.250.75*0.250.55
FS30A30*30.181.18*0.120.4
FS30B30*6.40.371.18*0.250.82
FS3535*80.541.38*0.311.19
FS3838*50.371.5*0.20.82
FS40A40*80.621.57*0.311.37
FS40B40*100.791.57*0.391.74
FS46B46*6.40.581.81*0.251.28
FS50A50*20.251.97*0.080.55
FS50B50*40.381.97*0.160.84
FS50C50*60.591.97*0.241.3
FS50D50*80.761.97*0.311.68
FS50E50*151.431.97*0.593.15
FS60A60*20.242.36*0.080.53
FS60B60*40.482.36*0.161.06
FS6464*4.80.62.52*0.191.32
FS7070*40.552.76*0.161.21
FS7676*9.51.422.99*0.373.13
FS100A100*101.953.94*0.394.3
FS100B100*254.853.94*0.9810.7
FS102A102*3.20.634.02*0.131.39
FS102B102*50.974.02*0.22.4
FS102C102*6.41.34.02*0.252.87
FS120120*102.44.72*0.395.29
FS152A152*102.925.98*0.396.44
FS152B152*205.95.98*0.7913
FS190190*155.427.48*0.5912
FS280280*105.3211.02*0.3911.7
FS300300*2414.411.81*0.9431.8
FS355355*53.513.98*0.27.72
FS555555*55.421.85*0.211.9
FS751751*57.229.57*0.215.9

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Standard color

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Grass green,Yellow, Grey, Orange

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

Grass green,Yellow, Grey

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

Grass green,Yellow, Grey

General acid and alkali environment

Application:

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.  

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

The structural flat bar is suitable for load-bearing and connecting parts that require strength and span, such as platform supports, handrails, walkway grating frames, equipment supports, and structural components in corrosive environments such as chemical and marine applications. Its glass fiber reinforced resin system has practical application value in situations requiring insulation, light weight, and corrosion resistance. For selection under specific working conditions, we recommend communicating with us to confirm based on load and medium conditions.

Selection Guidance

When selecting, mainly consider width, thickness, required load-bearing capacity, support span, and service environment. Different specifications in the table correspond to different moments of inertia and weights, which can be matched according to installation space and loading condition. If splicing, openings, or combination with other FRP components are involved, we recommend providing drawings or usage conditions. Please contact us for detailed specifications and selection advice.

Product Advantages

This flat bar is formed by the pultrusion process with continuous fiber distribution, offering high longitudinal strength and stiffness. It also has the common FRP characteristics of light weight, corrosion resistance, electrical insulation, and maintenance-free operation, and is easy to cut and install on site. Compared with traditional metal profiles, it can reduce rust and maintenance costs in corrosive or electromagnetically sensitive environments. Different surface treatments can be provided according to requirements.

Inquiry Guidance

To confirm specific specifications, length, surface treatment, and packaging method, please provide your application scenario and quantity requirements. We can recommend suitable models based on your project conditions. Please contact us for detailed specifications and quotations. We will arrange dedicated personnel to follow up and provide technical support.

Operating Environment

  • This pultruded FRP flat strip is built for both indoor and outdoor service, where the glass fiber reinforcement and resin matrix resist moisture and humidity without swelling or rusting.
  • In industrial plants and chemical processing areas, the flat strip withstands exposure to corrosive media such as acids, alkalis and salts, making it suitable for environments where steel would degrade.
  • As a structural profile for high-strength, large-span situations, it performs across a wide temperature range without losing dimensional stability.
  • Typical installations include walkways, platforms and support frames where the flat strip is exposed to weather, washdown or chemical splash.

立即联系我们,我们将有专业人员为您服务。

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send