Structural Profiles - Curved Flat Bar (Vinyl Ester)
Request a Quote
Please feel freely to contact with us for new price .
Genius FRP
FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.

Varieties | Size(mm) | Weight(kg/m) | Size(in) | Weight(lbs/in) |
|---|---|---|---|---|
Riglet radian | Width*Thickness | Width*Thickness | ||
| FS50A | 50*3.2 | 0.29 | 2" x 1/8" | 0.64 |
| FS60A | 60*3.2 | 0.36 | 19/8" x 1/8" | 0.79 |
| FS70 | 70*4 | 0.54 | 19" x 3/16" | 1.19 |
| FS90A | 90*3.2 | 0.54 | 7/2" x 1/8" | 1.19 |
| FS100 | 100*3.2 | 0.6 | 4" x 1/8" | 1.32 |
| FS120 | 120*3 | 0.7 | 19/4" x 1/8" | 1.54 |
Markets

Architectural
Bridge & Highway
Chemical
Food & Beverage
Manufacturing
Metals & Mining
Microelectronics
Oil & Gsa
Pharmaceutical
Power
Pulp & Paper
Recreation
Telecommunications
Transportation
Water & Wastewater
The characteristics:
Corrosion Resistant
Low Maintenance
Fire Retardant
Low Install Cost
Heavy Metal Safe
Long Service Life
Electrically & Thermally Non Conductive
High Strength-to-Weight Ratio
Introduction of raw materials——Resin type
Code | Resin type | Flame retardant property | Recommended usage occasions |
|---|---|---|---|
VEFR-25 | Vinyl type | Oxygen index 28 or above | Acid, alkali and other corrosive harsh environment |
IFR-25 | Meta benzene | Oxygen index 28 or above | A VEFR type economy, and excellent, moderate acid alkali and solvent |
OFR-25 | Ortho type | Oxygen index 28 or above | General acid and alkali environment |
Application:
Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.
Genius Shapes
Mechanical Properties | ASTM | Units | Value | Units | Value |
|---|---|---|---|---|---|
Tensile Stress, LW | D-638 | psi | 30000 | kgf/m² | 21092086 |
Tensile Stress, CW | D-638 | psi | 7000 | kgf/m² | 4921487 |
Tensile Modulus, LW | D-638 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Tensile Modulus, CW | D-638 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Compressive Stress, LW | D-695 | psi | 30000 | kgf/m² | 21092086 |
Compressive Stress, CW | D-695 | psi | 15000 | kgf/m² | 10546043 |
Compressive Modulus, LW | D-695 | 10^6psi | 2.5 | 10^6kgf/m² | 1758 |
Compressive Modulus, CW | D-695 | 10^6psi | 1 | 10^6kgf/m² | 703 |
Flexural Stress, LW | D-790 | psi | 30000 | kgf/m² | 21092086 |
Flexural Stress, CW | D-790 | psi | 10000 | kgf/m² | 7030695 |
Flexural Modulus, LW | D-790 | 10^6psi | 1.8 | 10^6kgf/m² | 1266 |
Flexural Modulus, CW | D-790 | 10^6psi | 0.8 | 10^6kgf/m² | 562 |
Modulus of Elasticity | Full Section | 10^6psi | 2.8 | 10^6kgf/m² | 1969 |
Shear Modulus | --- | 10^6psi | 0.45 | 10^6kgf/m² | 316 |
Short Beam Shear | D-2344 | psi | 4500 | kgf/m² | 3163813 |
Punch Shear | D-732 | psi | 10000 | kgf/m² | 7030695 |
Notched Izod Impact,LW | D-256 | ft.-lbs./in. | 25 | kg/m | 3.46 |
Notched Izod Impact,CW | D-256 | ft.-lbs./in. | 4 | kg/m | 0.55 |
Excludes Round Rod and Square Bar
Physical Properties | ASTM | Units | Value |
|---|---|---|---|
Barcoal | D-495 | --- | 45 |
24 Hour Water Absorption | D-570 | %max | 0.45 |
Density | D-792 | lbs./in.³ | 0.062-0.07 |
Coefficient of Thermal Expansion,LW | D-696 | 10^-6in./in./℃ | 8 |
Flammability Properties | ASTM | Units | Value |
|---|---|---|---|
Tunnel test* | E-84 | Flame Spread | 25 max |
Flammability* | D-635 | --- | Non-Burning |
Electrical Properties | ASTM | Units | Value |
|---|---|---|---|
Arc Resistance,LW | D-495 | seconds | 120 |
Dielectric Strength,LW | D-149 | kv./in. | 35 |
Dielectric Strength,PF | D-149 | volts/mil | 200 |
Dielectric Constant,PF | D-150 | @60hz | 5 |
LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face
*Pertains to ISOFR and VEFR only
Application Scenarios
Structural Profiles - Curved Flat Bar (Vinyl) is suitable for platforms, walkways, handrails and curved structural support applications requiring corrosion resistance and lightweight construction, and is often used in combination with grating and pultruded profiles. To confirm suitability under specific working conditions, please contact us for detailed specifications and selection advice.
Selection Guide
During selection, consider the arc radius, section width and thickness, load-bearing span and installation method, and pay attention to connection compatibility with adjacent components. As various specification combinations are involved, please contact us for detailed specifications and quotations, and our technical staff will assist in confirming the appropriate model.
Product Advantages
This profile is pultruded from glass fiber reinforced material and resin, featuring lightweight, high strength, corrosion resistance, insulation and dimensional stability, making it suitable for high-strength, large-span applications. The vinyl system helps improve resistance to chemical media, with specific performance varying with the service environment.
Inquiry Guide
If you need to know the available specification range, surface treatment options and delivery arrangements, please contact us for detailed specifications and quotations. Please provide the required section dimensions, arc requirements and service environment, and we will reply with a corresponding solution accordingly.
Operating Environment
- Vinyl ester FRP structural profiles are formulated for continuous outdoor exposure, resisting UV degradation and weathering in industrial and marine atmospheres.
- These pultruded profiles handle humid, wet and salt-laden conditions without the corrosion that affects steel, making them suitable for coastal, offshore and chemical plant environments.
- They withstand splashes and fumes from acids, alkalis and solvents where vinyl ester resin is specified, though direct contact with concentrated or high-temperature chemical streams should be confirmed against the project’s media list.
- Typical installations include walkways, platforms, handrails and cable trays in wastewater treatment, chemical processing and offshore structures, where the profile remains stable across outdoor temperature swings and condensing humidity.
简体中文