Structural Profiles - Angle (Orthophthalic)

Structural Profiles - Angle (Orthophthalic)

Price on request

Request a Quote


Please feel freely to contact with us for new price .

Genius FRP  

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Angle steel

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Angle steel

A*B*T1*T2
A*B*T1*T2
EL25A25*25*3.2*3.20.331" x 1" x 1/8" x 1/8"0.73
EL25B25*25*6.4*6.40.561" x 1" x 1/4" x 1/4"1.23
EL30A30*30*4(75°)0.46

5/4" x 5/4" x 3/16" (75°)

1.01
EL30B30*30*5*50.57

5/4" x 5/4" x 3/16" x 3/16"

1.26
EL3232*32*4*40.42

5/4" x 5/4" x 3/16" x 3/16"

0.93
EL38A38*38*5*50.68

3/2" x 3/2" x 3/16" x 3/16"

1.5
EL38B38*38*6.4*6.40.85

3/2" x 3/2" x 1/4" x 1/4"

1.87
EL4545*45*4.8*4.80.75

7/4" x 7/4" x 3/16" x 3/16"

1.65
EL50A50*50*3.2*3.20.62

2" x 2" x 1/8" x 1/8"

1.37
EL50B50*50*6.4*6.41.14

2" x 2" x 1/4" x 1/4"

2.51
EL6060*60*9*91.9

19/8" x 19/8" x 3/8" x 3/8"

4.19
EL76A76*76*4.8*4.81.38

3" x 3" x 3/16" x 3/16"

3.04
EL76B76*76*6.4*6.41.77

3" x 3" x 1/4" x 1/4"

3.9
EL76C76*76*9.5*9.52.57

3" x 3" x 3/8" x 3/8"

5.67
EL76D76*76*12.7*12.73.4

3" x 3" x 1/2" x 1/2"

7.5
EL101A101*101*6.4*6.42.5

4" x 4" x 1/4" x 1/4"

5.51
EL101B101*101*8*82.95

4" x 4" x 5/16" x 5/16"

6.5
EL101C101*101*9.5*9.53.48

4" x 4" x 3/8" x 3/8"

7.67
EL101D101*101*12.7*12.74.57

4" x 4" x 1/2" x 1/2"

10.1
EL152A152*152*6.4*6.43.62

6" x 6" x 1/4" x 1/4"

7.98
EL152B152*152*9.5*9.55.42

6" x 6" x 3/8" x 3/8"

12
EL152C152*152*12.7*12.77.01

6" x 6" x 1/2" x 1/2"

15.5
L4040*22*4.0*4.00.45

25/16" x 7/8" x 3/16" x 3/16"

0.99
L7676*15*6*60.98

3" x 9/16" x 1/4" x 1/4"

2.16
L100100*50*6.4*6.41.8

4" x 2" x 1/4" x 1/4"

3.97
L145145*76*10*103.85

23/4" x 3" x 3/8" x 3/8"

8.49
L170170*76*9.5*9.54.4

27/4" x 3" x 3/8" x 3/8"

9.7
L180180*80*8.0*8.03.89

7" x 25/8" x 5/16" x 5/16"

8.58
L254254*40*6.4*6.43.61

10" x 25/16" x 1/4" x 1/4"

7.96
L70(Special)70*70*24*6.03.75

11/4" x 11/4" x 15/16" x 1/4"

8.27

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

Application:

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.  

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

FRP angle is commonly used in chemical, wastewater treatment, marine engineering, power and general corrosive environments for platform supports, handrail frames, cable tray supports and structural reinforcement. Its ortho-type resin system suits most conventional industrial corrosive conditions; for strong acids, strong alkalis or high-temperature media, please contact us with your service environment so we can recommend a more suitable resin system.

Selection Guide

When selecting, first confirm equal or unequal leg, leg width and thickness, then determine the section size based on span, load direction and connection method; in the table, A*B*T1*T2 represent the two leg lengths and their corresponding thicknesses. As FRP is an anisotropic material, we recommend our assistance in checking load and deflection requirements before finalizing the model; contact us with your operating parameters for selection advice.

Product Advantages

Pultruded FRP angle uses glass fiber as reinforcement and resin as matrix, and is continuously pultruded and heat-cured to form. It features light weight, high strength, corrosion resistance, rust-free, non-magnetic and insulating properties, and is easy to cut and drill on site. Compared with traditional steel, it reduces maintenance and replacement frequency in corrosive environments, making it suitable for applications with both weight and durability requirements.

Inquiry Guide

For details on specifications, dimensional tolerances, surface treatment, packaging and delivery lead time of Structural Profiles - Angle (Ortho), please contact us for detailed specifications and a quotation. Please also provide the required model, quantity, service environment and delivery destination, and we will offer a tailored solution and commercial terms accordingly.

Operating Environment

  • This FRP angle steel uses orthophthalic resin and glass fiber reinforcement, so it is suited to outdoor and indoor structural framing where moisture and atmospheric exposure would corrode conventional steel angles.
  • Typical installations include chemical plants, water treatment areas and coastal or humid industrial sites, where the profile resists splash, vapour and mildly corrosive media without the rusting seen in metal angles.
  • The pultruded glass fiber construction keeps the angle stable across the normal service temperature range of industrial buildings and open-air structures, from cold workshops to sun-exposed platforms.
  • For continuous immersion, strong solvents or concentrated acids, or for load-bearing designs, contact us with your service conditions so the correct resin grade and profile can be confirmed.