Genius FRP  

  FRP structural shapes profile is made of glass fiber reinforced material, resin as adhesive, glass fiber cloth as a package reinforcement layer, through the thorough penetration, in the metal mold heating, molding, curing, drawing in the traction machine pulled A new type of composite material, with good physical properties, widely used in high strength, large span Situation.  

Angle steel

Varieties

Size(mm)

Weight(kg/m)

Size(in)

Weight(lbs/in)

Angle steel

A*B*T1*T2
A*B*T1*T2
EL25A25*25*3.2*3.20.331" x 1" x 1/8" x 1/8"0.73
EL25B25*25*6.4*6.40.561" x 1" x 1/4" x 1/4"1.23
EL30A30*30*4(75°)0.46

5/4" x 5/4" x 3/16" (75°)

1.01
EL30B30*30*5*50.57

5/4" x 5/4" x 3/16" x 3/16"

1.26
EL3232*32*4*40.42

5/4" x 5/4" x 3/16" x 3/16"

0.93
EL38A38*38*5*50.68

3/2" x 3/2" x 3/16" x 3/16"

1.5
EL38B38*38*6.4*6.40.85

3/2" x 3/2" x 1/4" x 1/4"

1.87
EL4545*45*4.8*4.80.75

7/4" x 7/4" x 3/16" x 3/16"

1.65
EL50A50*50*3.2*3.20.62

2" x 2" x 1/8" x 1/8"

1.37
EL50B50*50*6.4*6.41.14

2" x 2" x 1/4" x 1/4"

2.51
EL6060*60*9*91.9

19/8" x 19/8" x 3/8" x 3/8"

4.19
EL76A76*76*4.8*4.81.38

3" x 3" x 3/16" x 3/16"

3.04
EL76B76*76*6.4*6.41.77

3" x 3" x 1/4" x 1/4"

3.9
EL76C76*76*9.5*9.52.57

3" x 3" x 3/8" x 3/8"

5.67
EL76D76*76*12.7*12.73.4

3" x 3" x 1/2" x 1/2"

7.5
EL101A101*101*6.4*6.42.5

4" x 4" x 1/4" x 1/4"

5.51
EL101B101*101*8*82.95

4" x 4" x 5/16" x 5/16"

6.5
EL101C101*101*9.5*9.53.48

4" x 4" x 3/8" x 3/8"

7.67
EL101D101*101*12.7*12.74.57

4" x 4" x 1/2" x 1/2"

10.1
EL152A152*152*6.4*6.43.62

6" x 6" x 1/4" x 1/4"

7.98
EL152B152*152*9.5*9.55.42

6" x 6" x 3/8" x 3/8"

12
EL152C152*152*12.7*12.77.01

6" x 6" x 1/2" x 1/2"

15.5
L4040*22*4.0*4.00.45

25/16" x 7/8" x 3/16" x 3/16"

0.99
L7676*15*6*60.98

3" x 9/16" x 1/4" x 1/4"

2.16
L100100*50*6.4*6.41.8

4" x 2" x 1/4" x 1/4"

3.97
L145145*76*10*103.85

23/4" x 3" x 3/8" x 3/8"

8.49
L170170*76*9.5*9.54.4

27/4" x 3" x 3/8" x 3/8"

9.7
L180180*80*8.0*8.03.89

7" x 25/8" x 5/16" x 5/16"

8.58
L254254*40*6.4*6.43.61

10" x 25/16" x 1/4" x 1/4"

7.96
L70(Special)70*70*24*6.03.75

11/4" x 11/4" x 15/16" x 1/4"

8.27

Markets  

Markets

  • Architectural

  • Bridge & Highway

  • Chemical

  • Food & Beverage

  • Manufacturing

  • Metals & Mining

  • Microelectronics

  • Oil & Gsa

  • Pharmaceutical

  • Power

  • Pulp & Paper

  • Recreation

  • Telecommunications

  • Transportation

  • Water & Wastewater

The characteristics:

  • Corrosion Resistant

  • Low Maintenance

  • Fire Retardant

  • Low Install Cost

  • Heavy Metal Safe

  • Long Service Life

  • Electrically & Thermally Non Conductive

  • High Strength-to-Weight Ratio

Introduction of raw materials——Resin type

Code

Resin type

Flame retardant property

Recommended usage occasions

VEFR-25

Vinyl type

Oxygen index 28 or above

Acid, alkali and other corrosive harsh environment

IFR-25

Meta benzene

Oxygen index 28 or above

A VEFR type economy, and excellent, moderate acid alkali and solvent

OFR-25

Ortho type

Oxygen index 28 or above

General acid and alkali environment

Application:

  Genius© pultruded fiberglass structural shapes from Genius Composite Inc. are used in a wide range of applications and provide a unique combination of corrosion resistance, high strength, dimensional stability and light weight, along with thermal and electric non-conductivity. Durable Genius shapes provide years of low maintenance service in areas where steel, aluminum or wood components are traditionally specified. Today ,these shapes are often used in highly corrosive applications where stainless steel and other expensive components were once required.  

Genius Shapes

Mechanical Properties

ASTM

Units

Value

Units

Value

Tensile Stress, LW

D-638

psi

30000

kgf/m²

21092086

Tensile Stress, CW

D-638

psi

7000

kgf/m²

4921487

Tensile Modulus, LW

D-638

10^6psi

2.5

10^6kgf/m²

1758

Tensile Modulus, CW

D-638

10^6psi

0.8

10^6kgf/m²

562

Compressive Stress, LW

D-695

psi

30000

kgf/m²

21092086

Compressive Stress, CW

D-695

psi

15000

kgf/m²

10546043

Compressive Modulus, LW

D-695

10^6psi

2.5

10^6kgf/m²

1758

Compressive Modulus, CW

D-695

10^6psi

1

10^6kgf/m²

703

Flexural Stress, LW

D-790

psi

30000

kgf/m²

21092086

Flexural Stress, CW

D-790

psi

10000

kgf/m²

7030695

Flexural Modulus, LW

D-790

10^6psi

1.8

10^6kgf/m²

1266

Flexural Modulus, CW

D-790

10^6psi

0.8

10^6kgf/m²

562

Modulus of Elasticity

Full Section

10^6psi

2.8

10^6kgf/m²

1969

Shear Modulus

---

10^6psi

0.45

10^6kgf/m²

316

Short Beam Shear

D-2344

psi

4500

kgf/m²

3163813

Punch Shear

D-732

psi

10000

kgf/m²

7030695

Notched Izod Impact,LW

D-256

ft.-lbs./in.

25

kg/m

3.46

Notched Izod Impact,CW

D-256

ft.-lbs./in.

4

kg/m

0.55

  Excludes Round Rod and Square Bar

Physical Properties

ASTM

Units

Value

Barcoal

D-495

---

45

24 Hour Water Absorption

D-570

%max

0.45

Density

D-792

lbs./in.³

0.062-0.07

Coefficient of Thermal Expansion,LW

D-696

10^-6in./in./℃

8

Flammability Properties

ASTM

Units

Value

Tunnel test*

E-84

Flame Spread

25 max

Flammability*

D-635

---

Non-Burning

Electrical Properties

ASTM

Units

Value

Arc Resistance,LW

D-495

seconds

120

Dielectric Strength,LW

D-149

kv./in.

35

Dielectric Strength,PF

D-149

volts/mil

200

Dielectric Constant,PF

D-150

@60hz

5

LW=Lengthwise, CW=Crosswise,PF=Perpendicular to Laminate Face

*Pertains to ISOFR and VEFR only


Application Scenarios

Structural Profiles - Angle (Isophthalic) is suitable for corrosive environments such as chemical, marine and wastewater treatment, as well as structural support applications requiring high strength and long spans. The isophthalic resin provides excellent corrosion and weather resistance, maintaining stability during long-term use in outdoor and humid conditions. Contact us to learn about the suitability of this product for your specific project.

Selection Guide

When selecting, determine the angle size according to design loads, spans and connection methods. Different leg widths and thicknesses correspond to different load-bearing capacities, and the isophthalic resin type can meet higher corrosion resistance requirements. For precise selection advice, contact us for detailed specifications and technical support.

Product Advantages

Compared with traditional metal materials, FRP angles feature lightweight, high strength, corrosion resistance, insulation and non-magnetic properties, and are easy to cut and install. The isophthalic resin system further enhances the product's chemical resistance and durability, making it suitable for demanding industrial environments. Contact us for more information on product advantages.

Inquiry Guidance

For detailed specifications, prices and supply information on Structural Profiles - Angle (Isophthalic), please contact us. We can provide customized solutions according to your project requirements. Please submit your inquiry via the website or email, and we will reply as soon as possible.

Free,easy click for support

7*24 professional team support. Within 24 Hours, our team will give you the feedback.

Send   
 Website Visitor