LM Wire Rope GB 6X37 IWRC
Please feel freely to contact with us for new price .
Product Details
6x37 is a cross laid construction used for general engineering applications. 6x37 is also available with IWRC (independent wire rope core). In the UK 6x36 is a far more popular construction, whilst on the European mainland, vast quantities of 6x37 are used for a variety of applications.。
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006
.jpg?access_token=3cc09a22-9720-43d1-b58a-87a5548f102a)
Applications
General engineering applications
Crane ropes
Hoist rope
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 12 | 0.55 | 81.3 | 8293 | 90 | 9183 |
| 13 | 0.64 | 95.4 | 9733 | 106 | 10777 |
| 14 | 0.75 | 111 | 11288 | 123 | 12499 |
| 16 | 0.98 | 145 | 14743 | 160 | 16326 |
| 18 | 1.23 | 183 | 18659 | 203 | 20662 |
| 20 | 1.52 | 226 | 23036 | 250 | 25509 |
| 22 | 1.84 | 273 | 27874 | 302 | 30866 |
| 24 | 2.2 | 325 | 33173 | 360 | 36734 |
| 26 | 2.58 | 382 | 38932 | 423 | 43111 |
| 28 | 2.99 | 443 | 45152 | 490 | 49999 |
| 30 | 3.43 | 508 | 51833 | 563 | 57397 |
| 32 | 3.9 | 578 | 58974 | 640 | 65305 |
| 34 | 4.4 | 653 | 66576 | 723 | 73723 |
| 36 | 4.94 | 732 | 74639 | 810 | 82651 |
| 38 | 5.5 | 815 | 83163 | 903 | 92090 |
| 40 | 6.1 | 903 | 92147 | 1000 | 102039 |
| 42 | 6.72 | 996 | 101592 | 1103 | 112498 |
| 44 | 7.38 | 1093 | 111498 | 1211 | 123467 |
| 46 | 8.06 | 1195 | 121865 | 1323 | 134946 |
| 48 | 8.78 | 1301 | 132692 | 1441 | 146936 |
General Engineering Ropes
绿盟LM专门供应多股光面或镀锌钢丝绳。我们的产品直径从0.5mm到64mm不等,包括带纤维芯和钢芯的1X19、7X7、6X19、7X19、6X36、8X19、8X36、19X7和35X7各种规格。除这些常规钢丝绳外,我们还可以提供优质的特种钢丝绳。
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
请根据实际工况确认所需直径、表面处理(光面或镀锌)、绳芯结构(如 IWRC 独立钢丝绳芯)及破断荷载等级,并结合 6x37 与 6x36 等规格在不同地区的使用习惯进行选择。工程交叉铺设、起重与吊索等不同用途对柔韧性和耐磨性的要求不同,欢迎联系我们获取针对您项目的选型建议与详细规格。
产品优势
LM Wire Rope GB 6X37 IWRC 按国标 GB/T 20118-2006 生产,提供光面或镀锌表面处理,6x37 结构适用于工程交叉铺设,并可选 IWRC 独立钢丝绳芯以提升结构稳定性。产品覆盖通用工程钢丝绳、起重机钢丝绳与吊索等应用场景,欢迎联系我们了解详细规格与报价。
询盘引导
如需确认直径、表面处理、绳芯形式、破断荷载等技术参数,或获取报价与交期信息,欢迎联系我们。请提供您的应用场景与需求数量,我们将安排专人对接并提供详细规格与商务条款。
简体中文
English