LM Wire Rope GB 6X36 FC
Please feel freely to contact with us for new price .
Product Details
6x36 wire rope is a flexible general engineering wire rope available with either FC (fibre core) or IWRC (independent wire rope core). The wire rope has a superior breaking load and a good fatigue life. This wire rope can be used for a wide range of applications.
Surface treatment:Ungalv, Galvanized or Marine Grade Stainless Steel.
Standard:GB/T 20118-2006
.jpg?access_token=e3404de3-f380-4cdd-ba71-560d71062c64)
Applications
General engineering
Ropes for grab cranes
Wire rope slings
Crane ropes
Hoist rope
Winch ropes
Lifeboat falls
Mooring ropes
Pursing wires
Luffing ropes
- Tow ropes
Breaking Loads
|
|
Min Breaking Loads | Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 8 | 0.24 | 37.4 | 3813 | 41.4 | 4222 |
| 9 | 0.3 | 47.3 | 4825 | 52.4 | 5343 |
| 10 | 0.37 | 58.4 | 5957 | 64.7 | 6597 |
| 11 | 0.44 | 70.7 | 7209 | 78.3 | 7982 |
| 12 | 0.53 | 84.1 | 8579 | 93.1 | 9500 |
| 13 | 0.62 | 98.7 | 10068 | 109 | 11149 |
| 14 | 0.72 | 115 | 11677 | 127 | 12930 |
| 15 | 0.83 | 131 | 13405 | 146 | 14844 |
| 16 | 0.94 | 150 | 15252 | 166 | 16889 |
| 18 | 1.19 | 189 | 19303 | 210 | 21375 |
| 19 | 1.33 | 211 | 21507 | 234 | 23816 |
| 20 | 1.47 | 234 | 23831 | 259 | 26389 |
| 22 | 1.78 | 283 | 28835 | 313 | 31931 |
| 24 | 2.11 | 336 | 34317 | 373 | 38000 |
| 26 | 2.48 | 395 | 40274 | 437 | 44598 |
| 28 | 2.88 | 458 | 46709 | 507 | 51723 |
| 30 | 3.3 | 526 | 53620 | 582 | 59376 |
| 32 | 3.76 | 598 | 61008 | 662 | 67557 |
| 34 | 4.24 | 675 | 68872 | 748 | 76265 |
| 36 | 4.76 | 757 | 77213 | 838 | 85501 |
| 38 | 5.3 | 843 | 86030 | 934 | 95265 |
| 40 | 5.87 | 935 | 95325 | 1035 | 105557 |
| 42 | 6.47 | 1030 | 105095 | 1141 | 116377 |
| 44 | 7.11 | 1131 | 115343 | 1252 | 127724 |
| 46 | 7.77 | 1236 | 126067 | 1369 | 139600 |
| 48 | 8.46 | 1346 | 137268 | 1490 | 152003 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
6x36钢丝绳按国标GB/T 20118-2006生产,具柔性好、抗疲劳性能佳的特点,适合抓斗起重机、吊索、绞车及系泊等通用场景。选型时请结合所需直径、芯型(FC纤维芯或IWRC独立钢丝绳芯)、表面处理(光面、镀锌、316不锈钢)及实际断裂荷载需求综合确定。如对规格匹配有疑问,欢迎联系我们获取详细规格与报价。
产品优势
该钢丝绳结构兼顾柔韧性与承载能力,断裂荷载表现优良,使用寿命较长,适用于频繁弯曲与反复受力的工况。提供纤维芯与钢芯两种选择,并有光面、镀锌及316航海级不锈钢表面,可适应室内外、潮湿及腐蚀性环境。具体性能与配置请以实际询盘确认。
询盘引导
如您需要特定直径、芯型、表面处理或长度规格,欢迎联系我们获取详细规格与报价。我们可依据您的应用场景提供选型参考与技术支持,商业条款与交期以正式沟通为准。
简体中文