LM Sealed Wire Rope GB6X19(9/9/1) IWRC

LM Sealed Wire Rope GB6X19(9/9/1) IWRC

Engineering tool Wire rope selector

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Product Details

6x19 locked coil wire rope is available with FC (fiber core) and IWRC (independent wire rope core), offering excellent breaking load characteristics and a wide range of applications. For applications requiring higher abrasion resistance, 6x19 locked coil wire rope is more suitable than other 6x19 wire ropes.

Surface finish: bright or galvanized

Standard: GB/T 20118-2006

Greenlogy TEC GB Fully Locked Coil Wire Rope 6X19(9/9/1) IWRC

Engineering applications

  • Drilling line

  • Elevator hoisting rope

  • Wire rope slings

  • Luffing wire rope

  • Hoisting rope

  • Crane wire rope


  • Sand line, core line and swabbing line

  • Trawl fishing / ocean sweeping

  • Grounding rope / ground tow rope

  • Oil well / oilfield

  • Excavator rope / scraper rope

  • Fishing rope

  • Tow rope

Breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load


Diameter

Weight

(1770Mpa)

(1770Mpa)

(1960Mpa)

(1960Mpa)

mm

kg/m

KN

Kg

KN

Kg

100.463642769.87117
110.4876.2777684.48611
120.5890.7925510110248
130.681071086211812028
140.781241259713713949
150.91421446115716013
161.021611645317918219
181.32042082422623059
201.62522570827928468
221.943053110733834447
242.33633702040240994
262.74264344847248111
283.144945038954755798
303.65675784562864054
324.16456581471572879
344.627287429880782274
365.188178329690492238
385.78910928091008102771
406.410081028351116113874
427.0611121133761231125546

General Engineering Wire Rope

   Greenlogy TEC specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium special wire ropes.

Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes strive to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with assembly components such as thimbles, swaged terminals, wedge sockets and many others. We also offer customization; our engineering team can manufacture wire rope to your required specifications. All materials are certified, traceable and conform to ISO9001.


Selection Guide

Selection should take into account factors such as load requirements, operating environment, wear resistance and flexibility. The 6x19 fully locked coil wire rope is available with FC (fiber core) and IWRC (independent wire rope core), and with bright or galvanized surface treatment to suit different working conditions. For specific selection advice, please contact us; our technical team will provide professional guidance based on your application.

Product Advantages

The 6x19 fully locked coil wire rope is produced to the national standard GB/T 20118-2006, offering excellent breaking load characteristics. It is more wear-resistant than other 6x19 wire ropes, making it suitable for applications with high wear resistance requirements. Its structural design balances strength and flexibility, and it is widely used in drilling lines, elevator hoisting ropes, crane ropes and many other engineering fields.

Inquiry Guide

If you have any questions about the specifications, performance or applications of the 6x19 fully locked coil wire rope, or need detailed technical parameters and a quotation, please contact us at any time. Kindly provide your specific requirements (such as diameter, core type, surface treatment, length, etc.), and we will provide a customized solution.

Cut to Length

Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.

WhatsApp