18X7 stainless steel wire rope is a non-rotating construction available in diameters from 1.5mm through to 16mm.It is used where low rotation is required including davit and crane rope applications.
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Marine crane rope
Marine/Saltwater environment
Sewage treatment works
Wire rope slings
Davit ropes
Breaking Loads
Diameter
| Weight
|
Min Breaking Loads(1570Mpa)
|
Min Breaking Loads(1570Mpa)
|
mm | kg/m | KN |
Kg |
| 6 | 0.14 | 18.5 | 1887 |
| 8 | 0.26 | 33 | 3366 |
| 9 | 0.32 | 41.7 | 4253 |
| 10 | 0.4 | 51.5 | 5253 |
| 11 | 0.5 | 62.3 | 6354 |
| 12 | 0.58 | 74.2 | 7568 |
| 13 | 0.68 | 87.1 | 8884 |
| 14 | 0.8 | 101 | 10302 |
| 16 | 1.04 | 132 | 13464 |
| 18 | 1.32 | 167 | 17034 |
| 19 | 1.44 | 186 | 18972 |
| 20 | 1.62 | 206 | 21012 |
| 22 | 2.04 | 249 | 25398 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
LM旋转 resistant 钢丝绳(GB18X7(6/1))适用于船用起重机、海洋与海水环境、污水处理厂、钢丝绳吊索及吊绳等需要低旋转特性的场合。选型时请结合工况的载荷、使用环境、直径与长度、表面处理(光面或镀锌)以及钢丝绳结构等因素综合评估。欢迎联系我们,告知您的具体应用与参数要求,我们将协助您确认合适规格。
产品优势
LM旋转 resistant 钢丝绳(GB18X7(6/1))按国标GB/T 20118-2006生产,提供光面或镀锌表面处理选项,具备良好的抗旋转性能,适合对低旋转有要求的工程应用。其结构设计有助于在动态工况下保持稳定,降低因旋转导致的磨损风险。如需了解更详细的性能特点,欢迎与我们联系。
询盘引导
如需获取LM旋转 resistant 钢丝绳(GB18X7(6/1))的详细规格、报价或定制方案,欢迎联系我们。请提供所需直径、长度、表面处理及数量等信息,我们将尽快回复并提供专业支持。
简体中文
English