LM Filler Wire Rope GB6X19 (12/6+6F/1)FC
Please feel freely to contact with us for new price .
Product Details
6X19 filler (often referred to as 6X25) is available with both FC (fibre core) and IWRC (independent wire rope core). With a fibre core, 6X19 filler will generally achieve a superior fatigue life to the other 6X19 constructions. 6X19 filler wire rope can work from 1 tonne load up to 5 tonnes. It is used in the North Sea Oil industry .
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-20066

Applications
Drilling ropes
Elevator rope
Wire rope slings
Derricking ropes
Pendant ropes
Crane rope
Sand, coring and swabbing lines
Trawl wraps / Pelagic sweeps
Ground cables
Oil well / Oil field
Excavator rope / Scraper rope
Fishing rope
Drag ropes
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 14 | 0.7 | 114 | 11677 | 127 | 12930 |
| 16 | 0.92 | 150 | 15252 | 166 | 16889 |
| 18 | 1.16 | 189 | 19303 | 210 | 21375 |
| 20 | 1.44 | 234 | 23831 | 259 | 26389 |
| 22 | 1.74 | 283 | 28835 | 313 | 31931 |
| 24 | 2.07 | 336 | 34317 | 373 | 38000 |
| 26 | 2.43 | 395 | 40274 | 437 | 44598 |
| 28 | 2.82 | 458 | 46709 | 507 | 51723 |
| 30 | 3.23 | 526 | 53620 | 582 | 59376 |
| 32 | 3.68 | 598 | 61008 | 662 | 67556 |
| 34 | 4.15 | 675 | 68872 | 748 | 76265 |
| 36 | 4.65 | 757 | 77213 | 838 | 85501 |
| 38 | 5.18 | 843 | 86030 | 934 | 95265 |
| 40 | 5.74 | 935 | 95325 | 1035 | 105557 |
| 42 | 6.33 | 1030 | 105095 | 1141 | 116377 |
| 44 | 6.95 | 1131 | 115343 | 1252 | 127724 |
| 46 | 7.6 | 1236 | 126067 | 1369 | 139600 |
| 48 | 8.27 | 1346 | 137268 | 1490 | 152003 |
General Engineering Ropes
绿盟LM专门供应多股光面或镀锌钢丝绳。我们的产品直径从0.5mm到64mm不等,包括带纤维芯和钢芯的1X19、7X7、6X19、7X19、6X36、8X19、8X36、19X7和35X7各种规格。除这些常规钢丝绳外,我们还可以提供优质的特种钢丝绳。
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
选型时请先确认钢丝绳的使用场景、所需直径范围、表面处理(光面或镀锌)及绳芯类型(FC纤维芯或IWRC独立钢丝绳芯),再结合上表断裂荷载数据匹配安全系数。若工况涉及频繁弯曲、腐蚀环境或重载吊装,欢迎联系我们获取详细规格与报价,由技术人员协助确认合适结构。
产品优势
6X19填料钢丝绳采用纤维芯结构,柔韧性较好,在同等直径下通常具有较长的使用寿命,并可按需提供光面或镀锌表面处理,适应多种吊装与牵引工况。产品依据国标GB/T 20118-2006生产,覆盖钻绳、电梯绳、索具及油田用绳等应用。
询盘引导
如需了解具体直径、绳芯、表面处理及包装方式,欢迎联系我们获取详细规格与报价。请提供使用场景、所需直径范围与数量,我们将据此推荐合适型号并确认商务条款。