LM Filler Compacted Wire Rope GB6X19 (12/6+6F/1) IWRC
Please feel freely to contact with us for new price .
Product Details
6X19 filler compacted wire rope (often referred to as 6X25) is available with both FC (fibre core) and IWRC (independent wire rope core). 6X19 filler wire rope can work from 1 tonne load up to 5 tonnes. It is used in the North Sea Oil industry .
Surface treatment:Ungalv or Galvanized
Standard:GB/T 20118-2006

Applications
Drilling ropes
Elevator rope
Wire rope slings
Derricking ropes
Pendant ropes
Crane rope
Sand, coring and swabbing lines
Trawl wraps / Pelagic sweeps
Ground cables
Oil well / Oil field
Excavator rope / Scraper rope
Fishing rope
Drag ropes
Breaking Loads
|
| Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 14 | 0.78 | 124 | 12597 | 137 | 13949 |
| 16 | 1.02 | 161 | 16453 | 179 | 18219 |
| 18 | 1.3 | 204 | 20824 | 226 | 23059 |
| 20 | 1.6 | 252 | 25708 | 279 | 28468 |
| 22 | 1.94 | 305 | 31107 | 338 | 34447 |
| 24 | 2.3 | 363 | 37020 | 402 | 40994 |
| 26 | 2.7 | 426 | 43448 | 472 | 48111 |
| 28 | 3.14 | 494 | 50389 | 547 | 55798 |
| 30 | 3.6 | 567 | 57845 | 628 | 64054 |
| 32 | 4.1 | 645 | 65814 | 715 | 72879 |
| 34 | 4.62 | 728 | 74298 | 807 | 82274 |
| 36 | 5.18 | 817 | 83296 | 904 | 92238 |
| 38 | 5.78 | 910 | 92809 | 1008 | 102771 |
| 40 | 6.4 | 1008 | 102835 | 1116 | 113874 |
| 42 | 7.06 | 1112 | 113376 | 1231 | 125546 |
| 44 | 7.74 | 1220 | 124431 | 1351 | 137788 |
| 46 | 8.46 | 1333 | 136000 | 1476 | 150598 |
| 48 | 9.22 | 1452 | 148083 | 1608 | 163979 |
General Engineering Ropes
绿盟LM专门供应多股光面或镀锌钢丝绳。我们的产品直径从0.5mm到64mm不等,包括带纤维芯和钢芯的1X19、7X7、6X19、7X19、6X36、8X19、8X36、19X7和35X7各种规格。除这些常规钢丝绳外,我们还可以提供优质的特种钢丝绳。
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
选型时需结合额定载荷、使用工况与安全系数综合确定直径与结构,并核对捻向、表面处理等要求。若不确定具体规格,欢迎联系我们,由技术人员协助确认合适的型号。
产品优势
6X19压实填料钢丝绳(12/6+6F/1)采用压实股与独立钢丝绳芯(IWRC)结构,股间填充丝减少内部磨损,柔韧性与耐磨性兼顾,适用于频繁弯曲与重载工况。表面可选光面或镀锌,以满足不同环境下的使用需求。
询盘引导
如需了解详细技术参数、可选规格范围及商务条款,欢迎联系我们获取详细规格与报价。我们可根据您的使用场景提供选型建议与供货方案。