LM Fiber Core(FC) Wire Rope GB7X7 (6/1)

LM Fiber Core(FC) Wire Rope GB7X7 (6/1)

Engineering tool Wire rope selector

Price on request

Get a quote
Request a Quote


Please feel freely to contact with us for new price .

Product Details

The core of 7X7 rope is a steel wire rope core.Steel wire ropes with diameters from 0.5 mm to 2 mm are common, and the rope as a whole is flexible.

Surface treatment: galvanized steel and 316 marine-grade stainless steel.

Standard: GB/T 20118-2006

Greenlogy TEC GB Fiber Core Wire Rope 7X7 (6/1)

Engineering Applications

  • Construction Engineering Applications

  • Small-diameter wire rope slings

  • Guy wires

  • Fencing ropes

  • Slings

  • Garage door wire ropes

  • Fixed guy wires

  • Tagline ropes

  • Cable car ropes

Breaking load

Minimum breaking load

Minimum breaking load

Diameter

Weight

(1770Mpa) 

(1770Mpa) 

mm

kg/m

KN

Kg

10.0040.7678
20.0152.75280
30.0356.18630
40.06111120
50.117.21751
60.1424.72521
70.1933.73432
80.25444483
90.3155.65674
100.3868.77004
110.4783.18475
120.5598.910087
130.6511611838
140.7513513729
160.9817617932
181.2422322696
201.5427528019
221.8633233903
242.2139640348
262.646447353
283.0153854918
303.4661863044

General Engineering Wire Rope

    Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized steel wire rope. Our products range in diameter from 0.5 mm to 64 mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 in various specifications with fiber cores and steel cores. In addition to these conventional wire ropes, we can also supply premium special wire ropes.

Most wire ropes work under demanding conditions and must be resistant to crushing, bending fatigue and wear. All our wire ropes are engineered to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure that all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged ends and wedge sockets, as well as many other assembly components. We also offer customization services: our engineering team can manufacture wire ropes to your required specifications. All materials are certified, traceable and compliant with ISO9001.


Selection Guide

Please confirm the required rope diameter, core structure (such as 7X7 or 6/1), surface treatment (galvanized steel or 316 stainless steel), and whether it needs to comply with GB/T 20118-2006 according to the actual application. If you have specific requirements for breaking load, flexibility or corrosion resistance, please contact us to describe your working conditions, and our technical staff will assist in matching the specifications.

Product Advantages

This product uses a wire rope core structure. Within a diameter range of 0.5 mm to 2 mm, it is flexible overall, making it easy to bend and knot. It is suitable for many applications such as slings, guy wires, fencing ropes, and garage door ropes. The surface can optionally be galvanized steel or 316 marine-grade stainless steel, balancing strength and corrosion resistance with strong engineering adaptability.

Inquiry Guidance

If you need to know the weight, minimum breaking load, packaging method, or delivery lead time for a specific diameter, please contact us for detailed specifications and a quotation. Please provide the required rope diameter, material, surface treatment, and order quantity, and we will reply as soon as possible.

Operating Environment

  • Galvanized steel and 316 marine-grade stainless steel constructions of this LM Fiber Core (FC) Wire Rope GB7X7 (6/1) are intended for outdoor and indoor service where moisture and atmospheric corrosion are present, with the 316 stainless variant suited to marine and other aggressive conditions.
  • The flexible 7X7 strand core allows the rope to run over sheaves and through routing in fixed and moving assemblies such as guy wires, fencing ropes, tagline ropes, garage door wire ropes and small-diameter slings.
  • As a rope with a steel wire rope core in diameters from 0.5 mm to 2 mm, it is best protected from abrasive contact with sharp edges, and consistent lubrication is recommended to extend service life in humid or polluted atmospheres.
  • Contact Greenlogy TEC for guidance on selecting galvanized or 316 stainless construction for the specific temperature, humidity and corrosive media of your application.

Cut to Length

Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.

WhatsApp