LM Compacted Wire Rope GB6x36 (14/7+7/7/1) IWRC
Request a Quote
Please feel freely to contact with us for new price .
Product Details
6x36 wire rope is available with FC (fiber core) or IWRC (independent wire rope core), and is a universal flexible engineering wire rope. This wire rope offers excellent breaking load capacity and good fatigue resistance, with a long service life and wide application.
Surface treatment: bright or galvanized
Standard: GB/T 20118-2006
.jpg?access_token=7e2e70c1-d0ab-45c6-be1c-626fbcc145b1)
Engineering Applications
General engineering applications
Grab crane ropes
Wire rope slings
Crane ropes
Slings
Winch ropes
Lifeboat ropes
Mooring ropes
Seeker ropes
Luffing ropes
Traction ropes
Breaking load
|
|
Minimum breaking load |
Minimum breaking load |
Minimum breaking load |
|---|---|---|---|---|
Diameter | Weight |
(1770Mpa)
|
(1960Mpa) |
(2160Mpa)
|
mm | kg/m | KN |
KN | KN |
| 12 | 0.68 | 112 | 124 | 131 |
| 13 | 0.79 | 131 | 147 | 157 |
| 14 | 0.93 | 153 | 169 | 183 |
| 15 | 1.06 | 176 | 194 | 208 |
| 16 | 1.19 | 198 | 219 | 237 |
| 18 | 1.52 | 250 | 277 | 298 |
| 19 | 1.68 | 275 | 305 | 329 |
| 20 | 1.85 | 307 | 340 | 368 |
| 22 | 2.26 | 370 | 410 | 441 |
| 24 | 2.74 | 447 | 492 | 540 |
| 25 | 2.93 | 481 | 532 | 576 |
| 26 | 3.14 | 520 | 581 | 622 |
| 28 | 3.68 | 604 | 663 | 722 |
| 30 | 4.21 | 689 | 763 | 831 |
| 32 | 4.75 | 777 | 861 | 949 |
| 34 | 5.45 | 891 | 980 | 1070 |
| 35 | 5.71 | 933 | 1033 | 1131 |
| 36 | 6.09 | 992 | 1099 | 1192 |
General engineering wire rope
Greenlogy TEC (LM) specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium special wire ropes.
Most wire ropes work under demanding conditions and must withstand crushing, bending fatigue and abrasion. All our wire ropes strive to achieve a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged ends and wedge sockets, as well as many other assembly components. We also offer customization services, and our engineering team can manufacture wire rope to your required specifications. All materials are certified, traceable and compliant with ISO9001.
Selection Guide
When selecting, please determine the appropriate wire rope diameter and strength grade based on the load requirements, usage frequency and environmental conditions of the actual working conditions, combined with the minimum breaking load data in the table above. If you are unsure, please contact us for professional selection advice.
Product Advantages
This wire rope adopts a 6x36 structure, offering high flexibility and fatigue resistance, suitable for a variety of lifting and traction scenarios. The Independent Wire Rope Core (IWRC) design improves the overall breaking load capacity and extends service life.
Inquiry Guide
For specific specifications, prices, delivery times or other commercial terms, please feel free to contact us at any time. We will provide you with detailed quotations and customized services.
Operating Environment
- This GB6x36 compacted wire rope with IWRC is suited to outdoor engineering applications such as grab crane ropes, mooring ropes and luffing ropes, where it is exposed to weather and temperature changes.
- The rope is available with a bright or galvanized surface treatment; the galvanized option provides enhanced resistance to atmospheric moisture compared with the bright finish.
- Typical uses include wire rope slings and winch ropes in general engineering, where the rope may encounter dust, humidity and intermittent contact with water.
- For indoor applications such as traction ropes or seeker ropes in controlled plant conditions, the rope performs without exposure to corrosive media.
Cut to Length
Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.