32x7 compacted wire rope is available in galvanized and non-galvanized versions, plus additional sizes 34x7, 35x7 and 37x7. To meet your requirements for higher breaking load and better wear characteristics, we can apply surface treatment, lubrication, plastic coating and compaction.

Surface treatment: bright or galvanized

Standard: GB/T 20118-2006

Greenlogy TEC GB Compacted Rotation-Resistant Wire Rope 32X7 (6/1)

Engineering Applications

  • Offshore crane wire rope

  • Deck crane wire rope

  • Column crane wire rope

  • Lifting slings

  • Main hoist wire rope

  • Slings

Breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load

Minimum breaking load


Diameter 

Weight

(1770Mpa) 

(1770Mpa) 

(1960Mpa) 

(1960Mpa) 

mm

kg/m

kN

Kg

kN

Kg

80.32505100555610
110.695969010510710
120.711111132212312546
130.841321346414614892
140.971531560616917238
151.11741774819319686
161.251982019621922338
181.612552601028228764
191.82842896831532130
201.973103162034435088
222.363723794441242024

General engineering wire rope

   Greenlogy TEC specializes in supplying multi-strand bright or galvanized wire rope. Our products range in diameter from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 specifications with fiber core and steel core. In addition to these standard wire ropes, we can also supply premium specialty wire ropes.

Most wire ropes work under demanding conditions and must resist crushing, bending fatigue and wear. All our wire ropes are engineered to deliver a high performance level to extend service life and thereby improve end-user productivity. We therefore ensure all materials are produced in accordance with wire rope industry standards. Every wire rope can be supplied with fittings such as thimbles, swaged terminals and wedge sockets, as well as many other assembly components. We also offer customization services; our engineering team can manufacture wire rope to your required specifications. All materials are certified, traceable and conform to ISO9001.


Selection Guide

This product is available in a range of diameters from 8mm to 22mm, with bright or galvanized surface treatment options, suitable for offshore crane, deck crane and main hoist applications. Please contact us with your actual load requirements, operating environment and matching rigging to obtain targeted selection advice and detailed specification confirmation.

Product Advantages

The 32x7 compacted structure improves rotation resistance while maintaining flexibility, and galvanizing enhances corrosion resistance, making it suitable for lifting scenarios with high demands on stability and wear resistance. We can also provide customization options such as surface treatment, lubrication, plastic coating and compaction according to your requirements.

Inquiry Guidance

For detailed technical parameters, available specifications or commercial cooperation terms of this product, please contact us to obtain detailed specifications and a quotation. Please inform us of the required diameter, surface treatment method and operating conditions, and we will provide a suitable solution for you.

Cut to Length

Need rope in fixed lengths? We cut wire rope to your required segment lengths before delivery (e.g. 5 m x 4 pcs + 10 m x 2 pcs), with end treatment per your needs. Request cut-to-length rope.

WhatsApp