LM (Coating) Wire Rope GB6X36 IWRC
Please feel freely to contact with us for new price .
Product Details
6x36 wire rope is a flexible general engineering wire rope available with either FC (fibre core) or IWRC (independent wire rope core). The wire rope has a superior breaking load and a good fatigue life. This wire rope can be used for a wide range of applications.
表面处理:光面、镀锌或16航海级不锈钢或镀锌
Standard:GB/T 20118-2006

Applications
General engineering
Ropes for grab cranes
Wire rope slings
Crane ropes
Hoist rope
Winch ropes
Lifeboat falls
Mooring ropes
Pursing wires
Pursing wires
- Tow ropes
Breaking Loads
|
|
Min Breaking Loads |
Min Breaking Loads |
Min Breaking Loads | Min Breaking Loads |
Diameter | Weight |
(1770Mpa) |
(1770Mpa) |
(1960Mpa) |
(1960Mpa) |
mm | kg/m | KN | Kg | KN | Kg |
| 8 | 0.26 | 40.3 | 4113 | 44.7 | 4555 |
| 9 | 0.33 | 51 | 5206 | 56.5 | 5764 |
| 10 | 0.41 | 63 | 6427 | 69.8 | 7117 |
| 11 | 0.5 | 76.2 | 7776 | 84.4 | 8611 |
| 12 | 0.59 | 90.7 | 9255 | 101 | 10248 |
| 13 | 0.69 | 107 | 10862 | 118 | 12028 |
| 14 | 0.8 | 124 | 12597 | 137 | 13949 |
| 16 | 1.05 | 161 | 16453 | 179 | 18219 |
| 18 | 1.33 | 204 | 20824 | 226 | 23059 |
| 19 | 1.48 | 228 | 23202 | 252 | 25692 |
| 20 | 1.64 | 252 | 25708 | 279 | 28468 |
| 22 | 1.98 | 305 | 31107 | 338 | 34447 |
| 24 | 2.36 | 363 | 37020 | 402 | 40994 |
| 26 | 2.77 | 426 | 43448 | 472 | 48111 |
| 28 | 3.21 | 494 | 50389 | 547 | 55798 |
| 30 | 3.68 | 567 | 57845 | 628 | 64054 |
| 32 | 4.19 | 645 | 65814 | 715 | 72879 |
| 34 | 4.73 | 728 | 74298 | 807 | 82274 |
| 36 | 5.3 | 817 | 83296 | 904 | 92238 |
| 38 | 5.91 | 910 | 92809 | 1008 | 102771 |
| 40 | 6.54 | 1008 | 102835 | 1116 | 113874 |
| 42 | 7.22 | 1112 | 113376 | 1231 | 125546 |
| 44 | 7.92 | 1220 | 124431 | 1351 | 137788 |
General Engineering Ropes
GREENLOGY TEC(LM) specializes in supplying multiple strands of ungalvanised and galvanized steel wire ropes. Our products range from 0.5mm to 64mm, including 1X19, 7X7, 6X19, 7X19, 6X36, 8X19, 8X36, 19X7 and 35X7 with both Fibre Core and Steel Cores. In addition to these conventional steel wire ropes, we can also provide high-quality special steel wire ropes.
Most wire ropes are used in harsh conditions and must have resistance to extrusion, bending fatigue and abrasion. All of our wire ropes are guaranteed to achieve the highest level , maximizing the service life to increase the productivity of end users. We ensure that all materials are produced in accordance with the best standards in the wire rope industry. Each wire rope can be supplied with a thimble eyes, swaged ends and wedge sockets ,as well as many other assembly components.In addition, we also provide customized services, our team of engineers can manufacture wire ropes of your required specifications. All materials are certified, traceable, and comply with ISO9001 standards.
选型指导
该产品提供 FC 与 IWRC 两种芯型,表面可做光面、镀锌等处理,适用于不同工况。请根据承载需求、使用环境与配套滑轮直径等因素选型,欢迎联系我们获取详细规格与报价。
产品优势
6x36 结构兼顾柔韧性与抗疲劳性能,断裂荷载能力较强,适合频繁弯曲的起重与吊装场景。芯型与表面处理可按应用需求搭配,以适配不同工况。
询盘引导
如需特定直径、芯型、表面处理或长度,欢迎联系我们说明使用场景与要求。我们将协助确认合适规格并提供报价。